{"id":1635,"date":"2026-02-04T12:34:43","date_gmt":"2026-02-04T05:34:43","guid":{"rendered":"https:\/\/inoxcuongthinh.com\/so-sanh-ve-dep-kha-nang-hoan-thien-be-mat-inox-dong-nhom\/"},"modified":"2026-02-04T12:34:43","modified_gmt":"2026-02-04T05:34:43","slug":"so-sanh-ve-dep-kha-nang-hoan-thien-be-mat-inox-dong-nhom","status":"publish","type":"post","link":"https:\/\/inoxcuongthinh.com\/so-sanh-ve-dep-kha-nang-hoan-thien-be-mat-inox-dong-nhom\/","title":{"rendered":"So s\u00e1nh v\u1ebb \u0111\u1eb9p, kh\u1ea3 n\u0103ng ho\u00e0n thi\u1ec7n b\u1ec1 m\u1eb7t: Inox, \u0110\u1ed3ng, Nh\u00f4m"},"content":{"rendered":"\n\n<div class=\"kk-star-ratings kksr-auto kksr-align-left kksr-valign-top\"\n    data-payload='{&quot;align&quot;:&quot;left&quot;,&quot;id&quot;:&quot;1635&quot;,&quot;slug&quot;:&quot;default&quot;,&quot;valign&quot;:&quot;top&quot;,&quot;ignore&quot;:&quot;&quot;,&quot;reference&quot;:&quot;auto&quot;,&quot;class&quot;:&quot;&quot;,&quot;count&quot;:&quot;0&quot;,&quot;legendonly&quot;:&quot;&quot;,&quot;readonly&quot;:&quot;&quot;,&quot;score&quot;:&quot;0&quot;,&quot;starsonly&quot;:&quot;&quot;,&quot;best&quot;:&quot;5&quot;,&quot;gap&quot;:&quot;5&quot;,&quot;greet&quot;:&quot;\u0110\u00e1nh gi\u00e1&quot;,&quot;legend&quot;:&quot;0\\\/5 - (0 b\u00ecnh ch\u1ecdn)&quot;,&quot;size&quot;:&quot;24&quot;,&quot;title&quot;:&quot;So s\u00e1nh v\u1ebb \u0111\u1eb9p, kh\u1ea3 n\u0103ng ho\u00e0n thi\u1ec7n b\u1ec1 m\u1eb7t: Inox, \u0110\u1ed3ng, Nh\u00f4m&quot;,&quot;width&quot;:&quot;0&quot;,&quot;_legend&quot;:&quot;{score}\\\/{best} - ({count} {votes})&quot;,&quot;font_factor&quot;:&quot;1.25&quot;}'>\n            \n<div class=\"kksr-stars\">\n    \n<div class=\"kksr-stars-inactive\">\n            <div class=\"kksr-star\" data-star=\"1\" style=\"padding-right: 5px\">\n            \n\n<div class=\"kksr-icon\" style=\"width: 24px; height: 24px;\"><\/div>\n        <\/div>\n            <div class=\"kksr-star\" data-star=\"2\" style=\"padding-right: 5px\">\n            \n\n<div class=\"kksr-icon\" style=\"width: 24px; height: 24px;\"><\/div>\n        <\/div>\n            <div class=\"kksr-star\" data-star=\"3\" style=\"padding-right: 5px\">\n            \n\n<div class=\"kksr-icon\" style=\"width: 24px; height: 24px;\"><\/div>\n        <\/div>\n            <div class=\"kksr-star\" data-star=\"4\" style=\"padding-right: 5px\">\n            \n\n<div class=\"kksr-icon\" style=\"width: 24px; height: 24px;\"><\/div>\n        <\/div>\n            <div class=\"kksr-star\" data-star=\"5\" style=\"padding-right: 5px\">\n            \n\n<div class=\"kksr-icon\" style=\"width: 24px; height: 24px;\"><\/div>\n        <\/div>\n    <\/div>\n    \n<div class=\"kksr-stars-active\" style=\"width: 0px;\">\n            <div class=\"kksr-star\" style=\"padding-right: 5px\">\n            \n\n<div class=\"kksr-icon\" style=\"width: 24px; height: 24px;\"><\/div>\n        <\/div>\n            <div class=\"kksr-star\" style=\"padding-right: 5px\">\n            \n\n<div class=\"kksr-icon\" style=\"width: 24px; height: 24px;\"><\/div>\n        <\/div>\n            <div class=\"kksr-star\" style=\"padding-right: 5px\">\n            \n\n<div class=\"kksr-icon\" style=\"width: 24px; height: 24px;\"><\/div>\n        <\/div>\n            <div class=\"kksr-star\" style=\"padding-right: 5px\">\n            \n\n<div class=\"kksr-icon\" style=\"width: 24px; height: 24px;\"><\/div>\n        <\/div>\n            <div class=\"kksr-star\" style=\"padding-right: 5px\">\n            \n\n<div class=\"kksr-icon\" style=\"width: 24px; height: 24px;\"><\/div>\n        <\/div>\n    <\/div>\n<\/div>\n                \n\n<div class=\"kksr-legend\" style=\"font-size: 19.2px;\">\n            <span class=\"kksr-muted\">\u0110\u00e1nh gi\u00e1<\/span>\n    <\/div>\n    <\/div>\n<div class=\"custom-toc\">\n<div id=\"ez-toc-container\" class=\"ez-toc-v2_0_85 counter-hierarchy ez-toc-counter ez-toc-grey ez-toc-container-direction\">\n<div class=\"ez-toc-title-container\">\n<p class=\"ez-toc-title\" style=\"cursor:inherit\">Table of Contents<\/p>\n<span class=\"ez-toc-title-toggle\"><a href=\"#\" class=\"ez-toc-pull-right ez-toc-btn ez-toc-btn-xs ez-toc-btn-default ez-toc-toggle\" aria-label=\"Toggle Table of Content\"><span class=\"ez-toc-js-icon-con\"><span class=\"\"><span class=\"eztoc-hide\" style=\"display:none;\">Toggle<\/span><span class=\"ez-toc-icon-toggle-span\"><svg style=\"fill: #999;color:#999\" xmlns=\"http:\/\/www.w3.org\/2000\/svg\" class=\"list-377408\" width=\"20px\" height=\"20px\" viewBox=\"0 0 24 24\" fill=\"none\"><path d=\"M6 6H4v2h2V6zm14 0H8v2h12V6zM4 11h2v2H4v-2zm16 0H8v2h12v-2zM4 16h2v2H4v-2zm16 0H8v2h12v-2z\" fill=\"currentColor\"><\/path><\/svg><svg style=\"fill: #999;color:#999\" class=\"arrow-unsorted-368013\" xmlns=\"http:\/\/www.w3.org\/2000\/svg\" width=\"10px\" height=\"10px\" viewBox=\"0 0 24 24\" version=\"1.2\" baseProfile=\"tiny\"><path d=\"M18.2 9.3l-6.2-6.3-6.2 6.3c-.2.2-.3.4-.3.7s.1.5.3.7c.2.2.4.3.7.3h11c.3 0 .5-.1.7-.3.2-.2.3-.5.3-.7s-.1-.5-.3-.7zM5.8 14.7l6.2 6.3 6.2-6.3c.2-.2.3-.5.3-.7s-.1-.5-.3-.7c-.2-.2-.4-.3-.7-.3h-11c-.3 0-.5.1-.7.3-.2.2-.3.5-.3.7s.1.5.3.7z\"\/><\/svg><\/span><\/span><\/span><\/a><\/span><\/div>\n<nav><ul class='ez-toc-list ez-toc-list-level-1 ' ><ul class='ez-toc-list-level-3' ><li class='ez-toc-heading-level-3'><a class=\"ez-toc-link ez-toc-heading-1\" href=\"https:\/\/inoxcuongthinh.com\/so-sanh-ve-dep-kha-nang-hoan-thien-be-mat-inox-dong-nhom\/#Noi_dung_chinh\" >N\u1ed9i dung ch\u00ednh<\/a><\/li><\/ul><\/li><li class='ez-toc-page-1 ez-toc-heading-level-2'><a class=\"ez-toc-link ez-toc-heading-2\" href=\"https:\/\/inoxcuongthinh.com\/so-sanh-ve-dep-kha-nang-hoan-thien-be-mat-inox-dong-nhom\/#Cac_tieu_chi_danh_gia_%E2%80%9Cve_dep%E2%80%9D_va_kha_nang_hoan_thien_be_mat\" >C\u00e1c ti\u00eau ch\u00ed \u0111\u00e1nh gi\u00e1 \u201cv\u1ebb \u0111\u1eb9p\u201d v\u00e0 kh\u1ea3 n\u0103ng ho\u00e0n thi\u1ec7n b\u1ec1 m\u1eb7t<\/a><\/li><li class='ez-toc-page-1 ez-toc-heading-level-2'><a class=\"ez-toc-link ez-toc-heading-3\" href=\"https:\/\/inoxcuongthinh.com\/so-sanh-ve-dep-kha-nang-hoan-thien-be-mat-inox-dong-nhom\/#Inox_Thep_khong_gi_da_dang_hoan_thien_ben_mau_va_bao_tri_thap\" >Inox (Th\u00e9p kh\u00f4ng g\u1ec9): \u0111a d\u1ea1ng ho\u00e0n thi\u1ec7n, b\u1ec1n m\u00e0u v\u00e0 b\u1ea3o tr\u00ec th\u1ea5p<\/a><ul class='ez-toc-list-level-3' ><li class='ez-toc-heading-level-3'><a class=\"ez-toc-link ez-toc-heading-4\" href=\"https:\/\/inoxcuongthinh.com\/so-sanh-ve-dep-kha-nang-hoan-thien-be-mat-inox-dong-nhom\/#Mac_thep_va_anh_huong_den_tham_my\" >M\u00e1c th\u00e9p v\u00e0 \u1ea3nh h\u01b0\u1edfng \u0111\u1ebfn th\u1ea9m m\u1ef9<\/a><\/li><li class='ez-toc-page-1 ez-toc-heading-level-3'><a class=\"ez-toc-link ez-toc-heading-5\" href=\"https:\/\/inoxcuongthinh.com\/so-sanh-ve-dep-kha-nang-hoan-thien-be-mat-inox-dong-nhom\/#Cac_kieu_hoan_thien_tieu_chuan_va_thong_so_goi_y\" >C\u00e1c ki\u1ec3u ho\u00e0n thi\u1ec7n ti\u00eau chu\u1ea9n v\u00e0 th\u00f4ng s\u1ed1 g\u1ee3i \u00fd<\/a><\/li><li class='ez-toc-page-1 ez-toc-heading-level-3'><a class=\"ez-toc-link ez-toc-heading-6\" href=\"https:\/\/inoxcuongthinh.com\/so-sanh-ve-dep-kha-nang-hoan-thien-be-mat-inox-dong-nhom\/#Uu_%E2%80%93_nhuoc_diem_ve_tham_my\" >\u01afu \u2013 nh\u01b0\u1ee3c \u0111i\u1ec3m v\u1ec1 th\u1ea9m m\u1ef9<\/a><\/li><li class='ez-toc-page-1 ez-toc-heading-level-3'><a class=\"ez-toc-link ez-toc-heading-7\" href=\"https:\/\/inoxcuongthinh.com\/so-sanh-ve-dep-kha-nang-hoan-thien-be-mat-inox-dong-nhom\/#Goi_y_ung_dung_tham_my\" >G\u1ee3i \u00fd \u1ee9ng d\u1ee5ng th\u1ea9m m\u1ef9<\/a><\/li><\/ul><\/li><li class='ez-toc-page-1 ez-toc-heading-level-2'><a class=\"ez-toc-link ez-toc-heading-8\" href=\"https:\/\/inoxcuongthinh.com\/so-sanh-ve-dep-kha-nang-hoan-thien-be-mat-inox-dong-nhom\/#Nhom_nhe_nhieu_mau_qua_anod_hoa_be_mat_tinh_te_nhung_nhay_tray\" >Nh\u00f4m: nh\u1eb9, nhi\u1ec1u m\u00e0u qua anod h\u00f3a, b\u1ec1 m\u1eb7t tinh t\u1ebf nh\u01b0ng nh\u1ea1y tr\u1ea7y<\/a><ul class='ez-toc-list-level-3' ><li class='ez-toc-heading-level-3'><a class=\"ez-toc-link ez-toc-heading-9\" href=\"https:\/\/inoxcuongthinh.com\/so-sanh-ve-dep-kha-nang-hoan-thien-be-mat-inox-dong-nhom\/#Hop_kim_va_anh_huong_den_be_mat\" >H\u1ee3p kim v\u00e0 \u1ea3nh h\u01b0\u1edfng \u0111\u1ebfn b\u1ec1 m\u1eb7t<\/a><\/li><li class='ez-toc-page-1 ez-toc-heading-level-3'><a class=\"ez-toc-link ez-toc-heading-10\" href=\"https:\/\/inoxcuongthinh.com\/so-sanh-ve-dep-kha-nang-hoan-thien-be-mat-inox-dong-nhom\/#Cac_hoan_thien_chinh_tren_nhom\" >C\u00e1c ho\u00e0n thi\u1ec7n ch\u00ednh tr\u00ean nh\u00f4m<\/a><\/li><li class='ez-toc-page-1 ez-toc-heading-level-3'><a class=\"ez-toc-link ez-toc-heading-11\" href=\"https:\/\/inoxcuongthinh.com\/so-sanh-ve-dep-kha-nang-hoan-thien-be-mat-inox-dong-nhom\/#Uu_%E2%80%93_nhuoc_diem_tham_my\" >\u01afu \u2013 nh\u01b0\u1ee3c \u0111i\u1ec3m th\u1ea9m m\u1ef9<\/a><\/li><li class='ez-toc-page-1 ez-toc-heading-level-3'><a class=\"ez-toc-link ez-toc-heading-12\" href=\"https:\/\/inoxcuongthinh.com\/so-sanh-ve-dep-kha-nang-hoan-thien-be-mat-inox-dong-nhom\/#Goi_y_ung_dung_tham_my-2\" >G\u1ee3i \u00fd \u1ee9ng d\u1ee5ng th\u1ea9m m\u1ef9<\/a><\/li><\/ul><\/li><li class='ez-toc-page-1 ez-toc-heading-level-2'><a class=\"ez-toc-link ez-toc-heading-13\" href=\"https:\/\/inoxcuongthinh.com\/so-sanh-ve-dep-kha-nang-hoan-thien-be-mat-inox-dong-nhom\/#Dong_sac_am_%E2%80%9Csong%E2%80%9D_theo_thoi_gian_voi_patina_sang_trong_thu_cong\" >\u0110\u1ed3ng: s\u1eafc \u1ea5m, \u201cs\u1ed1ng\u201d theo th\u1eddi gian v\u1edbi patina, sang tr\u1ecdng th\u1ee7 c\u00f4ng<\/a><ul class='ez-toc-list-level-3' ><li class='ez-toc-heading-level-3'><a class=\"ez-toc-link ez-toc-heading-14\" href=\"https:\/\/inoxcuongthinh.com\/so-sanh-ve-dep-kha-nang-hoan-thien-be-mat-inox-dong-nhom\/#Vat_lieu_va_sac_do\" >V\u1eadt li\u1ec7u v\u00e0 s\u1eafc \u0111\u1ed9<\/a><\/li><li class='ez-toc-page-1 ez-toc-heading-level-3'><a class=\"ez-toc-link ez-toc-heading-15\" href=\"https:\/\/inoxcuongthinh.com\/so-sanh-ve-dep-kha-nang-hoan-thien-be-mat-inox-dong-nhom\/#Cac_hoan_thien_tieu_bieu\" >C\u00e1c ho\u00e0n thi\u1ec7n ti\u00eau bi\u1ec3u<\/a><\/li><li class='ez-toc-page-1 ez-toc-heading-level-3'><a class=\"ez-toc-link ez-toc-heading-16\" href=\"https:\/\/inoxcuongthinh.com\/so-sanh-ve-dep-kha-nang-hoan-thien-be-mat-inox-dong-nhom\/#Uu_%E2%80%93_nhuoc_diem_tham_my-2\" >\u01afu \u2013 nh\u01b0\u1ee3c \u0111i\u1ec3m th\u1ea9m m\u1ef9<\/a><\/li><\/ul><\/li><li class='ez-toc-page-1 ez-toc-heading-level-2'><a class=\"ez-toc-link ez-toc-heading-17\" href=\"https:\/\/inoxcuongthinh.com\/so-sanh-ve-dep-kha-nang-hoan-thien-be-mat-inox-dong-nhom\/#So_sanh_theo_tinh_huong_thuc_te\" >So s\u00e1nh theo t\u00ecnh hu\u1ed1ng th\u1ef1c t\u1ebf<\/a><\/li><li class='ez-toc-page-1 ez-toc-heading-level-2'><a class=\"ez-toc-link ez-toc-heading-18\" href=\"https:\/\/inoxcuongthinh.com\/so-sanh-ve-dep-kha-nang-hoan-thien-be-mat-inox-dong-nhom\/#Quy_trinh_chon_hoan_thien_be_mat_%E2%80%9Cdung_ngay_tu_dau%E2%80%9D\" >Quy tr\u00ecnh ch\u1ecdn ho\u00e0n thi\u1ec7n b\u1ec1 m\u1eb7t \u201c\u0111\u00fang ngay t\u1eeb \u0111\u1ea7u\u201d<\/a><\/li><li class='ez-toc-page-1 ez-toc-heading-level-2'><a class=\"ez-toc-link ez-toc-heading-19\" href=\"https:\/\/inoxcuongthinh.com\/so-sanh-ve-dep-kha-nang-hoan-thien-be-mat-inox-dong-nhom\/#Gia_cong_han_va_xu_ly_vet_anh_huong_tham_my\" >Gia c\u00f4ng, h\u00e0n v\u00e0 x\u1eed l\u00fd v\u1ebft \u1ea3nh h\u01b0\u1edfng th\u1ea9m m\u1ef9<\/a><\/li><li class='ez-toc-page-1 ez-toc-heading-level-2'><a class=\"ez-toc-link ez-toc-heading-20\" href=\"https:\/\/inoxcuongthinh.com\/so-sanh-ve-dep-kha-nang-hoan-thien-be-mat-inox-dong-nhom\/#Chi_phi_tuong_doi_va_nang_luc_hoan_thien_tai_Viet_Nam\" >Chi ph\u00ed t\u01b0\u01a1ng \u0111\u1ed1i v\u00e0 n\u0103ng l\u1ef1c ho\u00e0n thi\u1ec7n t\u1ea1i Vi\u1ec7t Nam<\/a><\/li><li class='ez-toc-page-1 ez-toc-heading-level-2'><a class=\"ez-toc-link ez-toc-heading-21\" href=\"https:\/\/inoxcuongthinh.com\/so-sanh-ve-dep-kha-nang-hoan-thien-be-mat-inox-dong-nhom\/#Ve_sinh_%E2%80%93_bao_tri_de_duy_tri_ve_dep\" >V\u1ec7 sinh \u2013 b\u1ea3o tr\u00ec \u0111\u1ec3 duy tr\u00ec v\u1ebb \u0111\u1eb9p<\/a><\/li><li class='ez-toc-page-1 ez-toc-heading-level-2'><a class=\"ez-toc-link ez-toc-heading-22\" href=\"https:\/\/inoxcuongthinh.com\/so-sanh-ve-dep-kha-nang-hoan-thien-be-mat-inox-dong-nhom\/#Ket_luan_chon_vat_lieu_theo_%E2%80%9Cngon_ngu_tham_my%E2%80%9D_va_vong_doi\" >K\u1ebft lu\u1eadn: ch\u1ecdn v\u1eadt li\u1ec7u theo \u201cng\u00f4n ng\u1eef th\u1ea9m m\u1ef9\u201d v\u00e0 v\u00f2ng \u0111\u1eddi<\/a><\/li><\/ul><\/nav><\/div>\n<h3><span class=\"ez-toc-section\" id=\"Noi_dung_chinh\"><\/span>N\u1ed9i dung ch\u00ednh<span class=\"ez-toc-section-end\"><\/span><\/h3>\n<ul>\n<li><a href=\"#toc-0-cac-tieu-chi-danh-gia-ve-dep-va-kha-nang-hoan-thie\">C\u00e1c ti\u00eau ch\u00ed \u0111\u00e1nh gi\u00e1 \u201cv\u1ebb \u0111\u1eb9p\u201d v\u00e0 kh\u1ea3 n\u0103ng ho\u00e0n thi\u1ec7n b\u1ec1 m\u1eb7t<\/a><\/li>\n<li><a href=\"#toc-1-inox-thep-khong-gi-da-dang-hoan-thien-ben-mau-va-b\">Inox (Th\u00e9p kh\u00f4ng g\u1ec9): \u0111a d\u1ea1ng ho\u00e0n thi\u1ec7n, b\u1ec1n m\u00e0u v\u00e0 b\u1ea3o tr\u00ec th\u1ea5p<\/a><\/li>\n<li><a href=\"#toc-2-nhom-nhe-nhieu-mau-qua-anod-hoa-be-mat-tinh-te-nhu\">Nh\u00f4m: nh\u1eb9, nhi\u1ec1u m\u00e0u qua anod h\u00f3a, b\u1ec1 m\u1eb7t tinh t\u1ebf nh\u01b0ng nh\u1ea1y tr\u1ea7y<\/a><\/li>\n<li><a href=\"#toc-3-dong-sac-am-song-theo-thoi-gian-voi-patina-sang-tr\">\u0110\u1ed3ng: s\u1eafc \u1ea5m, \u201cs\u1ed1ng\u201d theo th\u1eddi gian v\u1edbi patina, sang tr\u1ecdng th\u1ee7 c\u00f4ng<\/a><\/li>\n<li><a href=\"#toc-4-so-sanh-theo-tinh-huong-thuc-te\">So s\u00e1nh theo t\u00ecnh hu\u1ed1ng th\u1ef1c t\u1ebf<\/a><\/li>\n<li><a href=\"#toc-5-quy-trinh-chon-hoan-thien-be-mat-dung-ngay-tu-dau\">Quy tr\u00ecnh ch\u1ecdn ho\u00e0n thi\u1ec7n b\u1ec1 m\u1eb7t \u201c\u0111\u00fang ngay t\u1eeb \u0111\u1ea7u\u201d<\/a><\/li>\n<li><a href=\"#toc-6-gia-cong-han-va-xu-ly-vet-anh-huong-tham-my\">Gia c\u00f4ng, h\u00e0n v\u00e0 x\u1eed l\u00fd v\u1ebft \u1ea3nh h\u01b0\u1edfng th\u1ea9m m\u1ef9<\/a><\/li>\n<li><a href=\"#toc-7-chi-phi-tuong-doi-va-nang-luc-hoan-thien-tai-viet-\">Chi ph\u00ed t\u01b0\u01a1ng \u0111\u1ed1i v\u00e0 n\u0103ng l\u1ef1c ho\u00e0n thi\u1ec7n t\u1ea1i Vi\u1ec7t Nam<\/a><\/li>\n<li><a href=\"#toc-8-ve-sinh-bao-tri-de-duy-tri-ve-dep\">V\u1ec7 sinh \u2013 b\u1ea3o tr\u00ec \u0111\u1ec3 duy tr\u00ec v\u1ebb \u0111\u1eb9p<\/a><\/li>\n<li><a href=\"#toc-9-ket-luan-chon-vat-lieu-theo-ngon-ngu-tham-my-va-vo\">K\u1ebft lu\u1eadn: ch\u1ecdn v\u1eadt li\u1ec7u theo \u201cng\u00f4n ng\u1eef th\u1ea9m m\u1ef9\u201d v\u00e0 v\u00f2ng \u0111\u1eddi<\/a><\/li>\n<\/ul>\n<\/div>\n<p>Trong b\u1ed9 ch\u1ee7 \u0111\u1ec1 \u201c\u0110\u1eb7t l\u00ean b\u00e0n c\u00e2n\u201d gi\u1eefa Inox v\u00e0 c\u00e1c kim lo\u1ea1i kh\u00e1c, c\u00e2u h\u1ecfi nhi\u1ec1u k\u1ef9 s\u01b0 v\u00e0 x\u01b0\u1edfng quan t\u00e2m nh\u1ea5t l\u00e0: v\u1eadt li\u1ec7u n\u00e0o \u0111\u1eb9p h\u01a1n v\u00e0 ho\u00e0n thi\u1ec7n b\u1ec1 m\u1eb7t t\u1ed1t h\u01a1n? B\u00e0i vi\u1ebft n\u00e0y \u0111i th\u1eb3ng v\u00e0o so s\u00e1nh chuy\u00ean s\u00e2u gi\u1eefa Inox, \u0110\u1ed3ng v\u00e0 Nh\u00f4m v\u1ec1 th\u1ea9m m\u1ef9, c\u00e1c c\u00f4ng ngh\u1ec7 ho\u00e0n thi\u1ec7n, \u0111\u1ed9 b\u1ec1n m\u00e0u, b\u1ea3o tr\u00ec, v\u00e0 c\u00e1ch ghi r\u00f5 th\u00f4ng s\u1ed1 tr\u00ean b\u1ea3n v\u1ebd \u0111\u1ec3 ra \u0111\u00fang ch\u1ea5t l\u01b0\u1ee3ng mong mu\u1ed1n.<\/p>\n<h2 id=\"toc-0-cac-tieu-chi-danh-gia-ve-dep-va-kha-nang-hoan-thie\"><span class=\"ez-toc-section\" id=\"Cac_tieu_chi_danh_gia_%E2%80%9Cve_dep%E2%80%9D_va_kha_nang_hoan_thien_be_mat\"><\/span>C\u00e1c ti\u00eau ch\u00ed \u0111\u00e1nh gi\u00e1 \u201cv\u1ebb \u0111\u1eb9p\u201d v\u00e0 kh\u1ea3 n\u0103ng ho\u00e0n thi\u1ec7n b\u1ec1 m\u1eb7t<span class=\"ez-toc-section-end\"><\/span><\/h2>\n<p>&#8211; \u0110\u1ed9 b\u00f3ng\/\u0111\u1ed9 g\u01b0\u01a1ng: th\u1ec3 hi\u1ec7n b\u1eb1ng \u0111\u1ed9 nh\u00e1m b\u1ec1 m\u1eb7t (Ra, \u00b5m) v\u00e0 \u0111\u1ed9 b\u00f3ng quang h\u1ecdc (GU \u1edf g\u00f3c 60\u00b0).<br \/>\n&#8211; M\u00e0u s\u1eafc v\u00e0 t\u00ednh \u0111\u1ed3ng \u0111\u1ec1u: m\u00e0u t\u1ef1 nhi\u00ean, c\u00e1c t\u00f9y ch\u1ecdn m\u00e0u, \u0111\u1ed9 \u1ed5n \u0111\u1ecbnh m\u00e0u theo th\u1eddi gian\/UV.<br \/>\n&#8211; H\u1ecda ti\u1ebft\/texture: x\u01b0\u1edbc m\u1ecbn (No.4), hairline (HL), phun bi m\u1edd (bead blast), kh\u1eafc hoa v\u0103n, etching.<br \/>\n&#8211; Ch\u1ed1ng v\u00e2n tay v\u00e0 ch\u1ed1ng b\u1ea9n: \u0111\u1ed9 d\u1ec5 b\u00e1m d\u1ea5u tay, c\u00f3 th\u1ec3 ph\u1ee7 l\u1edbp ch\u1ed1ng v\u00e2n tay (AFP) hay kh\u00f4ng.<br \/>\n&#8211; H\u00e0n \u2013 c\u1eaft \u2013 u\u1ed1n c\u00f3 \u201c\u0111\u1eb9p\u201d kh\u00f4ng: kh\u1ea3 n\u0103ng x\u00f3a v\u1ebft nhi\u1ec7t, x\u01b0\u1edbc h\u00e0n, \u0111\u1ed3ng m\u00e0u sau gia c\u00f4ng.<br \/>\n&#8211; B\u1ec1n m\u00e0u\/\u0103n m\u00f2n theo m\u00f4i tr\u01b0\u1eddng: bi\u1ec3n, h\u00f3a ch\u1ea5t nh\u1eb9, n\u1ed9i th\u1ea5t kh\u00f4, ngo\u1ea1i th\u1ea5t n\u1eafng m\u01b0a.<br \/>\n&#8211; Kh\u1ea3 n\u0103ng s\u1eeda ch\u1eefa\/thay th\u1ebf: \u0111\u00e1nh b\u00f3ng l\u1ea1i, t\u00e1i x\u01b0\u1edbc, t\u00e1i ph\u1ee7.<br \/>\n&#8211; Chi ph\u00ed \u2013 lead time: \u0111\u1ed9 s\u1eb5n c\u00f3 quy tr\u00ecnh ho\u00e0n thi\u1ec7n t\u1ea1i Vi\u1ec7t Nam\/H\u00e0 N\u1ed9i.<\/p>\n<p>L\u01b0u \u00fd v\u1ec1 th\u01b0\u1edbc \u0111o: Ra c\u00e0ng nh\u1ecf th\u00ec b\u1ec1 m\u1eb7t c\u00e0ng \u201cg\u01b0\u01a1ng\u201d. T\u00e0i li\u1ec7u ti\u00eau chu\u1ea9n: ISO 1302 (k\u00fd hi\u1ec7u nh\u00e1m), ASTM A480\/EN 10088 (quy \u01b0\u1edbc ho\u00e0n thi\u1ec7n Inox), ISO 7599 (anod h\u00f3a nh\u00f4m). Ngu\u1ed3n tham kh\u1ea3o: Nickel Institute, SSINA (Specialty Steel Industry of North America), European Aluminium, Copper Development Association.<\/p>\n<h2 id=\"toc-1-inox-thep-khong-gi-da-dang-hoan-thien-ben-mau-va-b\"><span class=\"ez-toc-section\" id=\"Inox_Thep_khong_gi_da_dang_hoan_thien_ben_mau_va_bao_tri_thap\"><\/span>Inox (Th\u00e9p kh\u00f4ng g\u1ec9): \u0111a d\u1ea1ng ho\u00e0n thi\u1ec7n, b\u1ec1n m\u00e0u v\u00e0 b\u1ea3o tr\u00ec th\u1ea5p<span class=\"ez-toc-section-end\"><\/span><\/h2>\n<h3><span class=\"ez-toc-section\" id=\"Mac_thep_va_anh_huong_den_tham_my\"><\/span>M\u00e1c th\u00e9p v\u00e0 \u1ea3nh h\u01b0\u1edfng \u0111\u1ebfn th\u1ea9m m\u1ef9<span class=\"ez-toc-section-end\"><\/span><\/h3>\n<p>&#8211; Inox 201: kinh t\u1ebf, ch\u1ecbu \u0103n m\u00f2n k\u00e9m h\u01a1n, d\u1ec5 \u1ed1 tr\u00e0 \u1edf m\u00f4i tr\u01b0\u1eddng \u1ea9m\/bi\u1ec3n, l\u00e2u d\u00e0i \u1ea3nh h\u01b0\u1edfng th\u1ea9m m\u1ef9.<br \/>\n&#8211; Inox 304: c\u00e2n b\u1eb1ng th\u1ea9m m\u1ef9 \u2013 b\u1ec1n m\u00e0u \u2013 chi ph\u00ed, d\u00f9ng ph\u1ed5 bi\u1ebfn cho n\u1ed9i\/ngo\u1ea1i th\u1ea5t.<br \/>\n&#8211; Inox 316: b\u1ec1n \u0103n m\u00f2n v\u01b0\u1ee3t tr\u1ed9i (clorua\/bi\u1ec3n), gi\u1eef v\u1ebb \u0111\u1eb9p t\u1ed1t nh\u1ea5t ngo\u00e0i tr\u1eddi kh\u1eafc nghi\u1ec7t.<\/p>\n<h3><span class=\"ez-toc-section\" id=\"Cac_kieu_hoan_thien_tieu_chuan_va_thong_so_goi_y\"><\/span>C\u00e1c ki\u1ec3u ho\u00e0n thi\u1ec7n ti\u00eau chu\u1ea9n v\u00e0 th\u00f4ng s\u1ed1 g\u1ee3i \u00fd<span class=\"ez-toc-section-end\"><\/span><\/h3>\n<p>&#8211; 2B (c\u00e1n ngu\u1ed9i, m\u1ecbn m\u1edd): Ra ~0,30\u20130,50 \u00b5m. N\u1ec1n kinh t\u1ebf, d\u1ec5 v\u1ec7 sinh, ph\u1ed5 bi\u1ebfn trong c\u00f4ng nghi\u1ec7p.<br \/>\n&#8211; BA \u2013 Bright Annealed (\u1ee7 s\u00e1ng): Ra ~0,10\u20130,20 \u00b5m, b\u00f3ng s\u00e2u, ph\u1ea3n x\u1ea1 cao, d\u1ec5 l\u1ed9 v\u00e2n tay.<br \/>\n&#8211; No.4 (x\u01b0\u1edbc m\u1ecbn): Ra ~0,40\u20130,80 \u00b5m, gi\u1ea5u v\u1ebft tay t\u1ed1t h\u01a1n BA, th\u00e2n thi\u1ec7n v\u1edbi thang m\u00e1y, m\u1eb7t d\u1ef1ng n\u1ed9i th\u1ea5t.<br \/>\n&#8211; Hairline (HL \u2013 x\u01b0\u1edbc d\u1ecdc li\u00ean t\u1ee5c): Ra ~0,30\u20130,60 \u00b5m, sang tr\u1ecdng, \u201ck\u00e9o d\u00e0i\u201d kh\u00f4ng gian, d\u1ec5 \u0111\u1ed3ng nh\u1ea5t n\u1ebfu qu\u1ea3n h\u01b0\u1edbng v\u00e2n \u0111\u00fang.<br \/>\n&#8211; Bead blast (phun bi m\u1edd): Ra ~0,8\u20131,6 \u00b5m t\u00f9y c\u1ee1 h\u1ea1t, \u00e1nh m\u1edd m\u1ecbn, h\u1ea1n ch\u1ebf ch\u00f3i.<br \/>\n&#8211; No.8\/8K (g\u01b0\u01a1ng): Ra <0,05 \u00b5m, \u0111\u1ed9 b\u00f3ng cao nh\u1ea5t, cho bi\u1ec3n hi\u1ec7u, trang tr\u00ed cao c\u1ea5p.\n\nC\u00f4ng ngh\u1ec7 t\u0103ng gi\u00e1 tr\u1ecb th\u1ea9m m\u1ef9:\n- \u0110i\u1ec7n \u0111\u00e1nh b\u00f3ng (electropolish): gi\u1ea3m Ra th\u00eam ~30\u201350%, t\u0103ng \u0111\u1ed9 s\u00e1ng v\u00e0 kh\u1ea3 n\u0103ng ch\u1ed1ng \u0103n m\u00f2n b\u1ec1 m\u1eb7t.\n- PVD\/ion plating (TiN, TiCN, TiAlN\u2026): t\u1ea1o m\u00e0u v\u00e0ng, \u0111en, \u0111\u1ed3ng, h\u1ed3ng\u2026 b\u1ec1n m\u00e0u h\u01a1n s\u01a1n; n\u00ean k\u1ebft h\u1ee3p b\u1ec1 m\u1eb7t x\u01b0\u1edbc\/HL \u0111\u1ec3 gi\u1ea3m v\u00e2n tay.\n- Kh\u1eafc\/etching h\u00f3a h\u1ecdc ho\u1eb7c c\u01a1: t\u1ea1o hoa v\u0103n, logo b\u1ec1n m\u00e0u.\nNgu\u1ed3n: SSINA, Nickel Institute, ASTM A480\/EN 10088.\n\n\n\n<h3><span class=\"ez-toc-section\" id=\"Uu_%E2%80%93_nhuoc_diem_ve_tham_my\"><\/span>\u01afu \u2013 nh\u01b0\u1ee3c \u0111i\u1ec3m v\u1ec1 th\u1ea9m m\u1ef9<span class=\"ez-toc-section-end\"><\/span><\/h3>\n<p>\u01afu \u0111i\u1ec3m<br \/>\n&#8211; Ph\u1ed5 ho\u00e0n thi\u1ec7n r\u1ed9ng, t\u1eeb m\u1edd s\u00e2u \u0111\u1ebfn g\u01b0\u01a1ng; c\u00f3 th\u1ec3 k\u1ebft h\u1ee3p PVD, AFP.<br \/>\n&#8211; Gi\u1eef m\u00e0u t\u1ed1t, \u0111\u1eb7c bi\u1ec7t m\u00e1c 304\/316; d\u1ec5 v\u1ec7 sinh, s\u1eeda x\u01b0\u1edbc c\u1ee5c b\u1ed9 tr\u00ean b\u1ec1 m\u1eb7t x\u01b0\u1edbc\/HL.<br \/>\n&#8211; M\u1ed1i h\u00e0n c\u00f3 th\u1ec3 x\u1eed l\u00fd \u0111\u1eb9p: t\u1ea9y m\u1ed1i h\u00e0n (pickling), passivation x\u00f3a m\u00e0u nhi\u1ec7t.<\/p>\n<p>Nh\u01b0\u1ee3c \u0111i\u1ec3m<br \/>\n&#8211; BA\/g\u01b0\u01a1ng d\u1ec5 in v\u00e2n tay; c\u1ea7n AFP ho\u1eb7c ch\u1ecdn HL\/No.4 \u0111\u1ec3 \u201cgi\u1ea5u\u201d d\u1ea5u tay.<br \/>\n&#8211; Gia c\u00f4ng ho\u00e0n thi\u1ec7n \u0111\u00f2i h\u1ecfi m\u00e1y m\u00e0i\/\u0111\u00e1nh b\u00f3ng c\u00f4ng su\u1ea5t v\u00e0 tay ngh\u1ec1; chi ph\u00ed cao cho g\u01b0\u01a1ng 8K, PVD cao c\u1ea5p.<\/p>\n<h3><span class=\"ez-toc-section\" id=\"Goi_y_ung_dung_tham_my\"><\/span>G\u1ee3i \u00fd \u1ee9ng d\u1ee5ng th\u1ea9m m\u1ef9<span class=\"ez-toc-section-end\"><\/span><\/h3>\n<p>&#8211; N\u1ed9i th\u1ea5t cao c\u1ea5p, thang m\u00e1y: HL\/No.4, t\u00f9y ch\u1ecdn PVD v\u00e0ng\/\u0111en.<br \/>\n&#8211; Ngo\u1ea1i th\u1ea5t\/bi\u1ec3n hi\u1ec7u b\u1ec1n: 316 g\u01b0\u01a1ng 8K + AFP ho\u1eb7c HL + PVD.<br \/>\n&#8211; Th\u1ef1c ph\u1ea9m\/d\u01b0\u1ee3c: 2B\/No.4, \u0111i\u1ec7n \u0111\u00e1nh b\u00f3ng cho b\u1ed3n\/\u0111\u01b0\u1eddng \u1ed1ng.<br \/>\nNgu\u1ed3n: Nickel Institute \u2013 h\u01b0\u1edbng d\u1eabn ho\u00e0n thi\u1ec7n v\u00e0 v\u1ec7 sinh inox.<\/p>\n<h2 id=\"toc-2-nhom-nhe-nhieu-mau-qua-anod-hoa-be-mat-tinh-te-nhu\"><span class=\"ez-toc-section\" id=\"Nhom_nhe_nhieu_mau_qua_anod_hoa_be_mat_tinh_te_nhung_nhay_tray\"><\/span>Nh\u00f4m: nh\u1eb9, nhi\u1ec1u m\u00e0u qua anod h\u00f3a, b\u1ec1 m\u1eb7t tinh t\u1ebf nh\u01b0ng nh\u1ea1y tr\u1ea7y<span class=\"ez-toc-section-end\"><\/span><\/h2>\n<h3><span class=\"ez-toc-section\" id=\"Hop_kim_va_anh_huong_den_be_mat\"><\/span>H\u1ee3p kim v\u00e0 \u1ea3nh h\u01b0\u1edfng \u0111\u1ebfn b\u1ec1 m\u1eb7t<span class=\"ez-toc-section-end\"><\/span><\/h3>\n<p>&#8211; 5xxx (5052, 5005): \u0111\u1ecbnh h\u00ecnh t\u1ed1t, anod h\u00f3a m\u00e0u \u0111\u1ed3ng \u0111\u1ec1u, d\u00f9ng \u1ed1p m\u1eb7t d\u1ef1ng.<br \/>\n&#8211; 6xxx (6061, 6063): \u0111\u00f9n profile ki\u1ebfn tr\u00fac, anod t\u1ed1t, c\u01a1 t\u00ednh cao h\u01a1n cho khung\/k\u1ebft c\u1ea5u.<\/p>\n<h3><span class=\"ez-toc-section\" id=\"Cac_hoan_thien_chinh_tren_nhom\"><\/span>C\u00e1c ho\u00e0n thi\u1ec7n ch\u00ednh tr\u00ean nh\u00f4m<span class=\"ez-toc-section-end\"><\/span><\/h3>\n<p>&#8211; Anod h\u00f3a (ISO 7599): l\u1edbp oxit d\u00e0y 10\u201325 \u00b5m (AA10\u2013AA25), t\u0103ng c\u1ee9ng b\u1ec1 m\u1eb7t, b\u1ec1n m\u00e0u; m\u00e0u t\u1ef1 nhi\u00ean (b\u1ea1c), \u0111en, \u0111\u1ed3ng, v\u00e0ng\u2026 \u0110\u1ed9 m\u1edd \u2013 b\u00f3ng t\u00f9y ti\u1ec1n x\u1eed l\u00fd:<br \/>\n  &#8211; Brushed + anod: Ra ~0,20\u20130,40 \u00b5m, v\u00e2n x\u01b0\u1edbc r\u00f5, sang tr\u1ecdng.<br \/>\n  &#8211; Bead blast + anod: Ra ~0,8\u20131,6 \u00b5m, m\u1ecbn m\u1edd, \u0111\u1eb3ng c\u1ea5p \u201cmatte\u201d.<br \/>\n  &#8211; H\u00f3a b\u00f3ng (chemical brightening) + anod: t\u1ea1o hi\u1ec7u \u1ee9ng \u201cchrome-like\u201d, v\u1eabn k\u00e9m g\u01b0\u01a1ng inox v\u1ec1 chi\u1ec1u s\u00e2u ph\u1ea3n x\u1ea1.<br \/>\n&#8211; S\u01a1n t\u0129nh \u0111i\u1ec7n: ph\u1ed5 m\u00e0u r\u1ed9ng, texture \u0111a d\u1ea1ng (m\u1ecbn, nh\u00e1m, gi\u1ea3 g\u1ed7); \u0111\u1ed9 b\u1ec1n t\u00f9y b\u1ed9t s\u01a1n v\u00e0 x\u1eed l\u00fd b\u1ec1 m\u1eb7t (conversion coating).<br \/>\n&#8211; \u0110\u00e1nh b\u00f3ng g\u01b0\u01a1ng c\u01a1 h\u1ecdc: c\u00f3 th\u1ec3 \u0111\u1ea1t r\u1ea5t s\u00e1ng nh\u01b0ng d\u1ec5 x\u01b0\u1edbc; c\u1ea7n ph\u1ee7 trong su\u1ed1t \u0111\u1ec3 gi\u1eef \u0111\u1ed9 b\u00f3ng.<\/p>\n<h3><span class=\"ez-toc-section\" id=\"Uu_%E2%80%93_nhuoc_diem_tham_my\"><\/span>\u01afu \u2013 nh\u01b0\u1ee3c \u0111i\u1ec3m th\u1ea9m m\u1ef9<span class=\"ez-toc-section-end\"><\/span><\/h3>\n<p>\u01afu \u0111i\u1ec3m<br \/>\n&#8211; D\u1ea3i m\u00e0u r\u1ed9ng qua anod\/s\u01a1n; b\u1ec1 m\u1eb7t \u201cm\u1ecbn\u201d v\u00e0 hi\u1ec7n \u0111\u1ea1i, r\u1ea5t h\u1ee3p phong c\u00e1ch t\u1ed1i gi\u1ea3n.<br \/>\n&#8211; Tr\u1ecdng l\u01b0\u1ee3ng nh\u1eb9, thu\u1eadn ti\u1ec7n cho t\u1ea5m l\u1edbn, profile ph\u1ee9c t\u1ea1p, khe h\u1edf s\u1eafc n\u00e9t.<\/p>\n<p>Nh\u01b0\u1ee3c \u0111i\u1ec3m<br \/>\n&#8211; N\u1ec1n nh\u00f4m m\u1ec1m, d\u1ec5 x\u01b0\u1edbc l\u00f5i d\u01b0\u1edbi l\u1edbp ph\u1ee7; v\u1ebft x\u01b0\u1edbc kh\u00f3 \u201cd\u1eb7m\u201d \u0111\u1ed3ng m\u00e0u sau anod.<br \/>\n&#8211; M\u1ed1i h\u00e0n \u0111\u1ec3 l\u1ea1i v\u00f9ng nhi\u1ec7t kh\u00e1c m\u00e0u, kh\u00f3 che n\u1ebfu kh\u00f4ng s\u01a1n ph\u1ee7 to\u00e0n b\u1ed9.<br \/>\n&#8211; M\u00e0u nhu\u1ed9m anod c\u00f3 th\u1ec3 phai nh\u1eb9 theo th\u1eddi gian n\u1ebfu ch\u1ea5t l\u01b0\u1ee3ng nhu\u1ed9m\/sealing k\u00e9m; c\u1ea7n nh\u00e0 anod uy t\u00edn.<br \/>\nNgu\u1ed3n: ISO 7599, European Aluminium \u2013 H\u01b0\u1edbng d\u1eabn ki\u1ebfn tr\u00fac.<\/p>\n<h3><span class=\"ez-toc-section\" id=\"Goi_y_ung_dung_tham_my-2\"><\/span>G\u1ee3i \u00fd \u1ee9ng d\u1ee5ng th\u1ea9m m\u1ef9<span class=\"ez-toc-section-end\"><\/span><\/h3>\n<p>&#8211; M\u1eb7t d\u1ef1ng, lam, tr\u1ea7n: anod AA20\u2013AA25, ti\u1ec1n x\u1eed l\u00fd bead blast ho\u1eb7c brushed \u0111\u1ed3ng nh\u1ea5t theo h\u01b0\u1edbng.<br \/>\n&#8211; N\u1ed9i th\u1ea5t, signage hi\u1ec7n \u0111\u1ea1i: anod \u0111en m\u1edd, b\u1ea1c m\u1edd; ho\u1eb7c s\u01a1n t\u0129nh \u0111i\u1ec7n m\u1ecbn si\u00eau m\u1edd.<br \/>\n&#8211; H\u1ea1n ch\u1ebf d\u00f9ng g\u01b0\u01a1ng nh\u00f4m cho b\u1ec1 m\u1eb7t d\u1ec5 va qu\u1ec7t; n\u1ebfu c\u1ea7n, ph\u1ee7 l\u1edbp trong su\u1ed1t c\u1ee9ng.<\/p>\n<h2 id=\"toc-3-dong-sac-am-song-theo-thoi-gian-voi-patina-sang-tr\"><span class=\"ez-toc-section\" id=\"Dong_sac_am_%E2%80%9Csong%E2%80%9D_theo_thoi_gian_voi_patina_sang_trong_thu_cong\"><\/span>\u0110\u1ed3ng: s\u1eafc \u1ea5m, \u201cs\u1ed1ng\u201d theo th\u1eddi gian v\u1edbi patina, sang tr\u1ecdng th\u1ee7 c\u00f4ng<span class=\"ez-toc-section-end\"><\/span><\/h2>\n<h3><span class=\"ez-toc-section\" id=\"Vat_lieu_va_sac_do\"><\/span>V\u1eadt li\u1ec7u v\u00e0 s\u1eafc \u0111\u1ed9<span class=\"ez-toc-section-end\"><\/span><\/h3>\n<p>&#8211; \u0110\u1ed3ng \u0111\u1ecf (C110): m\u00e0u \u0111\u1ecf \u1ea5m, c\u00f3 th\u1ec3 \u0111\u00e1nh g\u01b0\u01a1ng r\u1ea5t \u0111\u1eb9p.<br \/>\n&#8211; H\u1ecd \u0111\u1ed3ng (\u0111\u1ed3ng thau\/brass; \u0111\u1ed3ng thi\u1ebfc\/bronze): ph\u1ed5 s\u1eafc t\u1eeb v\u00e0ng, n\u00e2u, oliu; th\u01b0\u1eddng g\u1ecdi chung l\u00e0 \u201c\u0111\u1ed3ng\u201d trong n\u1ed9i th\u1ea5t.<\/p>\n<h3><span class=\"ez-toc-section\" id=\"Cac_hoan_thien_tieu_bieu\"><\/span>C\u00e1c ho\u00e0n thi\u1ec7n ti\u00eau bi\u1ec3u<span class=\"ez-toc-section-end\"><\/span><\/h3>\n<p>&#8211; \u0110\u00e1nh b\u00f3ng g\u01b0\u01a1ng: Ra <0,05 \u00b5m, ph\u1ea3n x\u1ea1 \u1ea5m, chi\u1ec1u s\u00e2u th\u1ecb gi\u00e1c cao; d\u1ec5 b\u00e1m v\u00e2n tay.\n- Patina t\u1ef1 nhi\u00ean\/ho\u00e1 h\u1ecdc: n\u00e2u, xanh r\u00eau, \u0111en than\u2026 t\u1ea1o \u201cv\u1ebb c\u1ed5 \u0111i\u1ec3n\u201d v\u00e0 \u0111\u1ed9c b\u1ea3n; c\u00f3 th\u1ec3 wax\/clear coat \u0111\u1ec3 c\u1ed1 \u0111\u1ecbnh t\u00f4ng.\n- Texturing th\u1ee7 c\u00f4ng: b\u00faa, kh\u1eafc, d\u1eadp hoa v\u0103n \u2013 t\u0103ng chi\u1ec1u s\u00e2u th\u1ea9m m\u1ef9.\n- Ph\u1ee7 b\u1ea3o v\u1ec7: s\u01a1n b\u00f3ng m\u1edd, nano-ceramic, s\u00e1p ong \u0111\u1ec3 gi\u1ea3m oxy h\u00f3a qu\u00e1 nhanh.\nNgu\u1ed3n: Copper Development Association \u2013 Finishes &#038; Patination.\n\n\n\n<h3><span class=\"ez-toc-section\" id=\"Uu_%E2%80%93_nhuoc_diem_tham_my-2\"><\/span>\u01afu \u2013 nh\u01b0\u1ee3c \u0111i\u1ec3m th\u1ea9m m\u1ef9<span class=\"ez-toc-section-end\"><\/span><\/h3>\n<p>\u01afu \u0111i\u1ec3m<br \/>\n&#8211; S\u1eafc \u1ea5m \u0111\u1eb7c tr\u01b0ng, patina \u201ck\u1ec3 chuy\u1ec7n th\u1eddi gian\u201d, r\u1ea5t n\u1ed5i b\u1eadt \u1edf kh\u00f4ng gian cao c\u1ea5p.<br \/>\n&#8211; D\u1ec5 t\u1ea1o ho\u00e0n thi\u1ec7n th\u1ee7 c\u00f4ng \u0111\u1ed9c \u0111\u00e1o, \u0111\u1ed9 \u201cartisan\u201d cao.<\/p>\n<p>Nh\u01b0\u1ee3c \u0111i\u1ec3m<br \/>\n&#8211; Nh\u1ea1y tr\u1ea7y x\u01b0\u1edbc v\u00e0 bi\u1ebfn m\u00e0u; c\u1ea7n b\u1ea3o tr\u00ec \u0111\u1ecbnh k\u1ef3 n\u1ebfu mu\u1ed1n gi\u1eef t\u00f4ng ban \u0111\u1ea7u.<br \/>\n&#8211; Kh\u00f4ng th\u00edch h\u1ee3p ti\u1ebfp x\u00fac th\u1ef1c ph\u1ea9m\/axit n\u1ebfu kh\u00f4ng c\u00f3 l\u1edbp l\u00f3t; mu\u1ed1i\/\u1ea9m c\u00f3 th\u1ec3 \u0111\u1ec3 l\u1ea1i v\u1ec7t loang.<br \/>\n&#8211; Kh\u00f3 \u0111\u1ed3ng m\u00e0u di\u1ec7n t\u00edch l\u1edbn, \u0111\u1eb7c bi\u1ec7t sau h\u00e0n\/gh\u00e9p.<br \/>\nNgu\u1ed3n: Copper Development Association.<\/p>\n<h2 id=\"toc-4-so-sanh-theo-tinh-huong-thuc-te\"><span class=\"ez-toc-section\" id=\"So_sanh_theo_tinh_huong_thuc_te\"><\/span>So s\u00e1nh theo t\u00ecnh hu\u1ed1ng th\u1ef1c t\u1ebf<span class=\"ez-toc-section-end\"><\/span><\/h2>\n<p>&#8211; C\u1ea7n b\u1ec1 m\u1eb7t g\u01b0\u01a1ng b\u1ec1n ngo\u00e0i tr\u1eddi:<br \/>\n  &#8211; T\u1ed1t nh\u1ea5t: Inox 316 g\u01b0\u01a1ng 8K + AFP ho\u1eb7c HL + PVD; gi\u1eef b\u00f3ng l\u00e2u, \u00edt phai.<br \/>\n  &#8211; Nh\u00f4m g\u01b0\u01a1ng: s\u00e1ng nh\u01b0ng d\u1ec5 x\u01b0\u1edbc; c\u00e2n nh\u1eafc ch\u1ec9 cho n\u1ed9i th\u1ea5t \u00edt ch\u1ea1m.<br \/>\n  &#8211; \u0110\u1ed3ng g\u01b0\u01a1ng: \u0111\u1eb9p nh\u01b0ng b\u1ea3o tr\u00ec cao; n\u00ean d\u00f9ng cho \u0111i\u1ec3m nh\u1ea5n nh\u1ecf.<br \/>\n&#8211; C\u1ea7n b\u1ea3ng m\u00e0u \u0111a d\u1ea1ng, \u0111\u1ed3ng \u0111\u1ec1u tr\u00ean di\u1ec7n r\u1ed9ng:<br \/>\n  &#8211; Nh\u00f4m anod\/s\u01a1n t\u0129nh \u0111i\u1ec7n l\u00e0 l\u1ef1a ch\u1ecdn s\u1ed1 1; m\u00e0u \u0111\u1ed3ng \u0111\u1ec1u, nh\u1eb9, l\u1eafp \u0111\u1eb7t nhanh.<br \/>\n  &#8211; Inox PVD c\u00f3 m\u00e0u sang nh\u01b0ng t\u1ed1n k\u00e9m h\u01a1n; kh\u00f3 m\u00e0u \u201c\u0111\u1ed3ng \u0111\u1ec1u tuy\u1ec7t \u0111\u1ed1i\u201d tr\u00ean di\u1ec7n r\u1ea5t l\u1edbn.<br \/>\n  &#8211; \u0110\u1ed3ng patina l\u00e0 \u201cm\u1ed7i t\u1ea5m m\u1ed9t v\u1ebb\u201d, c\u1ed1 \u00fd kh\u00f4ng \u0111\u1ed3ng nh\u1ea5t.<br \/>\n&#8211; Y\u00eau c\u1ea7u \u201cgi\u1ea5u v\u00e2n tay\u201d, \u00edt b\u1ea3o tr\u00ec:<br \/>\n  &#8211; Inox No.4\/HL, bead blast; c\u00f3 th\u1ec3 th\u00eam AFP.<br \/>\n  &#8211; Nh\u00f4m anod m\u1edd\/brushed m\u1ecbn.<br \/>\n  &#8211; \u0110\u1ed3ng: d\u00f9ng wax\/clear coat m\u1edd, ch\u1ea5p nh\u1eadn patina d\u1ea7n.<br \/>\n&#8211; Ven bi\u1ec3n\/\u1ea9m m\u1eb7n:<br \/>\n  &#8211; Inox 316 HL\/No.4, passivation sau gia c\u00f4ng, v\u1ec7 sinh \u0111\u1ecbnh k\u1ef3 ch\u1ed1ng tea staining.<br \/>\n  &#8211; Nh\u00f4m anod AA25, sealing t\u1ed1t, ch\u1ecdn h\u1ee3p kim 5xxx ch\u1ea5t l\u01b0\u1ee3ng ki\u1ebfn tr\u00fac.<br \/>\n  &#8211; \u0110\u1ed3ng: patina \u0111\u1eb9p nh\u01b0ng c\u00f3 th\u1ec3 ch\u1ea3y v\u1ec7t \u201crun-off\u201d tr\u00ean t\u01b0\u1eddng s\u00e1ng, c\u1ea7n thi\u1ebft k\u1ebf m\u00e1ng h\u1ee9ng\/n\u1eb9p.<br \/>\n&#8211; Th\u1ef1c ph\u1ea9m \u2013 d\u01b0\u1ee3c \u2013 y t\u1ebf:<br \/>\n  &#8211; Inox 304\/316 (2B\/No.4, electropolish) l\u00e0 ti\u00eau chu\u1ea9n.<br \/>\n  &#8211; Nh\u00f4m: d\u00f9ng ch\u1ecdn l\u1ecdc, tr\u00e1nh m\u00f4i tr\u01b0\u1eddng ki\u1ec1m m\u1ea1nh; kh\u00f4ng \u01b0u ti\u00ean v\u00f9ng CIP m\u1ea1nh.<br \/>\n  &#8211; \u0110\u1ed3ng: kh\u00f4ng khuy\u1ebfn ngh\u1ecb ti\u1ebfp x\u00fac th\u1ef1c ph\u1ea9m\/axit tr\u1ef1c ti\u1ebfp.<\/p>\n<h2 id=\"toc-5-quy-trinh-chon-hoan-thien-be-mat-dung-ngay-tu-dau\"><span class=\"ez-toc-section\" id=\"Quy_trinh_chon_hoan_thien_be_mat_%E2%80%9Cdung_ngay_tu_dau%E2%80%9D\"><\/span>Quy tr\u00ecnh ch\u1ecdn ho\u00e0n thi\u1ec7n b\u1ec1 m\u1eb7t \u201c\u0111\u00fang ngay t\u1eeb \u0111\u1ea7u\u201d<span class=\"ez-toc-section-end\"><\/span><\/h2>\n<p>1) X\u00e1c \u0111\u1ecbnh ng\u1eef c\u1ea3nh: trong nh\u00e0\/ngo\u00e0i tr\u1eddi\/ven bi\u1ec3n, m\u1ee9c \u0111\u1ed9 ch\u1ea1m tay, y\u00eau c\u1ea7u ph\u1ea3n x\u1ea1 cao hay m\u1edd.<br \/>\n2) Ch\u1ecdn n\u1ec1n v\u1eadt li\u1ec7u:<br \/>\n   &#8211; \u01afu ti\u00ean b\u1ec1n m\u00e0u \u2013 b\u1ea3o tr\u00ec th\u1ea5p: Inox 304\/316.<br \/>\n   &#8211; \u01afu ti\u00ean m\u00e0u \u0111a d\u1ea1ng \u2013 nh\u1eb9: Nh\u00f4m (5xxx\/6xxx).<br \/>\n   &#8211; \u01afu ti\u00ean s\u1eafc \u1ea5m \u201cs\u1ed1ng\u201d: \u0110\u1ed3ng\/\u0111\u1ed3ng thau.<br \/>\n3) Ch\u1ecdn ho\u00e0n thi\u1ec7n m\u1ee5c ti\u00eau:<br \/>\n   &#8211; Inox: HL h\u1ea1t 180\u2013240; No.4; 8K; bead blast; PVD; AFP; electropolish.<br \/>\n   &#8211; Nh\u00f4m: brushed + anod AA20\u201325; bead blast + anod; s\u01a1n t\u0129nh \u0111i\u1ec7n; chemical brightening.<br \/>\n   &#8211; \u0110\u1ed3ng: mirror + clear; patina h\u00f3a h\u1ecdc + wax\/nano.<br \/>\n4) L\u1ea5y m\u1eabu th\u1ef1c t\u1ebf kh\u1ed5 \u2265300\u00d7300 mm, ch\u1ec9 \u0111\u1ecbnh h\u01b0\u1edbng v\u00e2n.<br \/>\n5) Ghi tr\u00ean b\u1ea3n v\u1ebd\/spec:<br \/>\n   &#8211; Inox: \u201cSUS304, HL grit 240, Ra 0,4\u20130,6 \u00b5m, PVD TiN Gold, l\u1edbp AFP; m\u1ed1i h\u00e0n pickling + passivation.\u201d<br \/>\n   &#8211; Nh\u00f4m: \u201cAA5005, brushed 240 + anod sulfuric AA20, m\u00e0u \u0111en m\u1edd, sealing n\u00f3ng DI, \u0111\u1ed3ng m\u00e0u batch.\u201d<br \/>\n   &#8211; \u0110\u1ed3ng: \u201cC110, mirror Ra <0,05 \u00b5m, patina n\u00e2u \u0111\u1eadm \u0111\u1ed3ng \u0111\u1ec1u c\u1ea5p m\u1eabu, clear coat m\u1edd 2K.\u201d\n6) Ki\u1ec3m so\u00e1t ch\u1ea5t l\u01b0\u1ee3ng: \u0111o Ra, ki\u1ec3m GU, ki\u1ec3m batch-color; test mu\u1ed1i x\u1ecbt (n\u1ebfu c\u1ea7n), test lau v\u00e2n tay.\n7) K\u1ebf ho\u1ea1ch b\u1ea3o tr\u00ec: dung d\u1ecbch ph\u00f9 h\u1ee3p, t\u1ea7n su\u1ea5t, h\u01b0\u1edbng d\u1eabn lau theo v\u00e2n; tr\u00e1nh clo\/ki\u1ec1m m\u1ea1nh.\n\n\n\n<h2 id=\"toc-6-gia-cong-han-va-xu-ly-vet-anh-huong-tham-my\"><span class=\"ez-toc-section\" id=\"Gia_cong_han_va_xu_ly_vet_anh_huong_tham_my\"><\/span>Gia c\u00f4ng, h\u00e0n v\u00e0 x\u1eed l\u00fd v\u1ebft \u1ea3nh h\u01b0\u1edfng th\u1ea9m m\u1ef9<span class=\"ez-toc-section-end\"><\/span><\/h2>\n<p>&#8211; H\u01b0\u1edbng v\u00e2n: lu\u00f4n s\u1eafp x\u1ebfp chi ti\u1ebft theo c\u00f9ng h\u01b0\u1edbng x\u01b0\u1edbc\/HL; \u0111\u00e1nh s\u1ed1 m\u1eb7t tr\u01b0\u1edbc \u2013 sau \u0111\u1ec3 tr\u00e1nh l\u1ed9n m\u1eb7t.<br \/>\n&#8211; C\u1eaft laser \u2013 bavia: Inox c\u1ea7n m\u00e0i m\u00e9p h\u1ea1t 180\u2013240 tr\u01b0\u1edbc khi x\u01b0\u1edbc ho\u00e0n thi\u1ec7n; Nh\u00f4m d\u00f9ng \u0111\u00e1\/nh\u00e1m ch\u1ed1ng b\u1ebft, c\u00f3 dung d\u1ecbch b\u00f4i tr\u01a1n; \u0110\u1ed3ng d\u00f9ng nh\u00e1m m\u1ecbn, tr\u00e1nh \u201cb\u00f4i\u201d b\u1ec1 m\u1eb7t.<br \/>\n&#8211; H\u00e0n:<br \/>\n  &#8211; Inox: TIG\/MIG \u0111\u1ec3 l\u1ea1i v\u1ec7t nhi\u1ec7t; x\u1eed l\u00fd pickling + passivation \u0111\u1ec3 x\u00f3a \u1ed1 v\u00e0ng; m\u00e0i \u2013 ho\u00e0n thi\u1ec7n l\u1ea1i c\u00f9ng grit.<br \/>\n  &#8211; Nh\u00f4m: v\u00f9ng nhi\u1ec7t c\u00f3 th\u1ec3 kh\u00e1c m\u00e0u sau anod; gi\u1ea3i ph\u00e1p l\u00e0 s\u01a1n ph\u1ee7 to\u00e0n b\u1ed9 ho\u1eb7c d\u00f9ng thi\u1ebft k\u1ebf gi\u1ea5u m\u1ed1i h\u00e0n.<br \/>\n  &#8211; \u0110\u1ed3ng: h\u00e0n\/braze \u0111\u1ed5i t\u00f4ng; th\u01b0\u1eddng ho\u00e0n thi\u1ec7n patina\/clear coat sau c\u00f9ng \u0111\u1ec3 c\u00e2n b\u1eb1ng m\u00e0u.<br \/>\nNgu\u1ed3n: Nickel Institute (weld discoloration &#038; cleaning), SSINA.<\/p>\n<h2 id=\"toc-7-chi-phi-tuong-doi-va-nang-luc-hoan-thien-tai-viet-\"><span class=\"ez-toc-section\" id=\"Chi_phi_tuong_doi_va_nang_luc_hoan_thien_tai_Viet_Nam\"><\/span>Chi ph\u00ed t\u01b0\u01a1ng \u0111\u1ed1i v\u00e0 n\u0103ng l\u1ef1c ho\u00e0n thi\u1ec7n t\u1ea1i Vi\u1ec7t Nam<span class=\"ez-toc-section-end\"><\/span><\/h2>\n<p>&#8211; Kinh t\u1ebf nh\u1ea5t cho b\u1ec1 m\u1eb7t m\u1edd\/nh\u00e1m \u0111\u1ed3ng \u0111\u1ec1u: Nh\u00f4m anod\/s\u01a1n t\u0129nh \u0111i\u1ec7n.<br \/>\n&#8211; Trung \u2013 cao c\u1ea5p, b\u1ec1n m\u00e0u, \u201c\u0103n ti\u1ec1n\u201d \u1edf chi ti\u1ebft: Inox HL\/No.4, bead blast; PVD t\u0103ng chi ph\u00ed nh\u01b0ng sang tr\u1ecdng.<br \/>\n&#8211; Ngh\u1ec7 thu\u1eadt\/th\u1ee7 c\u00f4ng cao, \u0111i\u1ec3m nh\u1ea5n: \u0110\u1ed3ng patina ho\u1eb7c \u0111\u1ed3ng g\u01b0\u01a1ng + clear.<br \/>\n&#8211; Lead time:<br \/>\n  &#8211; Inox HL\/No.4: ph\u1ed5 bi\u1ebfn, nhanh; 8K\/PVD: l\u00e2u h\u01a1n do c\u00f4ng \u0111o\u1ea1n ph\u1ee5.<br \/>\n  &#8211; Nh\u00f4m anod: ph\u1ee5 thu\u1ed9c batch m\u00e0u v\u00e0 chi\u1ec1u d\u00e0i b\u1ec3; n\u00ean g\u1ed9p l\u00f4.<br \/>\n  &#8211; \u0110\u1ed3ng patina: c\u1ea7n th\u1eddi gian th\u1eed \u2013 kh\u00f3a m\u00e0u theo m\u1eabu.<\/p>\n<h2 id=\"toc-8-ve-sinh-bao-tri-de-duy-tri-ve-dep\"><span class=\"ez-toc-section\" id=\"Ve_sinh_%E2%80%93_bao_tri_de_duy_tri_ve_dep\"><\/span>V\u1ec7 sinh \u2013 b\u1ea3o tr\u00ec \u0111\u1ec3 duy tr\u00ec v\u1ebb \u0111\u1eb9p<span class=\"ez-toc-section-end\"><\/span><\/h2>\n<p>&#8211; Inox: lau \u0111\u1ecbnh k\u1ef3 b\u1eb1ng kh\u0103n m\u1ec1m + dung d\u1ecbch trung t\u00ednh pH~7; tr\u00e1nh clo\/axit m\u1ea1nh; v\u1edbi BA\/g\u01b0\u01a1ng d\u00f9ng kh\u0103n microfiber; v\u1ebft tr\u00e0\/\u1ed1 mu\u1ed1i: dung d\u1ecbch chuy\u00ean d\u1ee5ng kh\u00f4ng ch\u1ee9a clorua, sau \u0111\u00f3 r\u1eeda s\u1ea1ch, lau kh\u00f4. Ngu\u1ed3n: Nickel Institute \u2013 Cleaning Stainless Steel.<br \/>\n&#8211; Nh\u00f4m: tr\u00e1nh ki\u1ec1m m\u1ea1nh\/axit m\u1ea1nh l\u00e0m m\u1edd anod; lau n\u01b0\u1edbc s\u1ea1ch + x\u00e0 ph\u00f2ng nh\u1eb9; s\u01a1n t\u0129nh \u0111i\u1ec7n d\u00f9ng ch\u1ea5t t\u1ea9y pH trung t\u00ednh; kh\u00f4ng ch\u00e0 nh\u00e1m c\u1ee5c b\u1ed9 tr\u00ean anod nhu\u1ed9m.<br \/>\n&#8211; \u0110\u1ed3ng: n\u1ebfu mu\u1ed1n \u201cgi\u1eef m\u1edbi\u201d, d\u00f9ng s\u00e1p ong\/clear coat; n\u1ebfu ch\u1ea5p nh\u1eadn patina, v\u1ec7 sinh kh\u00f4, kh\u00f4ng d\u00f9ng amoniac\/axit m\u1ea1nh l\u00e0m loang; b\u1ea3o tr\u00ec l\u1ea1i l\u1edbp ph\u1ee7 theo chu k\u1ef3.<\/p>\n<h2 id=\"toc-9-ket-luan-chon-vat-lieu-theo-ngon-ngu-tham-my-va-vo\"><span class=\"ez-toc-section\" id=\"Ket_luan_chon_vat_lieu_theo_%E2%80%9Cngon_ngu_tham_my%E2%80%9D_va_vong_doi\"><\/span>K\u1ebft lu\u1eadn: ch\u1ecdn v\u1eadt li\u1ec7u theo \u201cng\u00f4n ng\u1eef th\u1ea9m m\u1ef9\u201d v\u00e0 v\u00f2ng \u0111\u1eddi<span class=\"ez-toc-section-end\"><\/span><\/h2>\n<p>&#8211; Inox l\u00e0 \u201cvua\u201d v\u1ec1 \u0111\u1ed9 b\u1ec1n m\u00e0u \u2013 ph\u1ed5 ho\u00e0n thi\u1ec7n \u2013 b\u1ea3o tr\u00ec th\u1ea5p. HL\/No.4 cho b\u1ec1 m\u1eb7t sang, gi\u1ea5u v\u00e2n tay; 8K + PVD cho \u0111i\u1ec3m nh\u1ea5n cao c\u1ea5p, \u0111\u1eb7c bi\u1ec7t v\u1edbi 304\/316 ngo\u00e0i tr\u1eddi.<br \/>\n&#8211; Nh\u00f4m n\u1ed5i tr\u1ed9i v\u1ec1 m\u00e0u s\u1eafc \u0111\u1ed3ng \u0111\u1ec1u v\u00e0 c\u1ea3m gi\u00e1c m\u1ecbn hi\u1ec7n \u0111\u1ea1i nh\u1edd anod\/s\u01a1n; nh\u1eb9, d\u1ec5 thi c\u00f4ng t\u1ea5m l\u1edbn, nh\u01b0ng nh\u1ea1y tr\u1ea7y v\u00e0 kh\u00f3 d\u1eb7m m\u00e0u c\u1ee5c b\u1ed9.<br \/>\n&#8211; \u0110\u1ed3ng mang l\u1ea1i s\u1eafc \u1ea5m, patina \u201cs\u1ed1ng\u201d theo th\u1eddi gian \u2013 ph\u00f9 h\u1ee3p kh\u00f4ng gian sang tr\u1ecdng, th\u1ee7 c\u00f4ng \u2013 \u0111\u1ed5i l\u1ea1i l\u00e0 b\u1ea3o tr\u00ec v\u00e0 ki\u1ec3m so\u00e1t \u0111\u1ed3ng m\u00e0u kh\u00f3 h\u01a1n.<\/p>\n<p>N\u1ebfu \u01b0u ti\u00ean b\u1ec1n \u0111\u1eb9p, \u00edt b\u1ea3o tr\u00ec v\u00e0 \u0111\u1ed3ng nh\u1ea5t l\u00e2u d\u00e0i: ch\u1ecdn Inox 304\/316 v\u1edbi ho\u00e0n thi\u1ec7n HL\/No.4 ho\u1eb7c g\u01b0\u01a1ng + AFP. N\u1ebfu \u01b0u ti\u00ean b\u1ea3ng m\u00e0u v\u00e0 c\u00e2n n\u1eb7ng: Nh\u00f4m anod\/s\u01a1n. N\u1ebfu mu\u1ed1n d\u1ea5u \u1ea5n ngh\u1ec7 thu\u1eadt v\u00e0 ch\u1ea5t li\u1ec7u \u201cs\u1ed1ng\u201d: \u0110\u1ed3ng\/patina. Cu\u1ed1i c\u00f9ng, h\u00e3y ch\u1ed1t b\u1eb1ng m\u1eabu th\u1eadt v\u00e0 ch\u1ec9 \u0111\u1ecbnh th\u00f4ng s\u1ed1 Ra, grit, l\u1edbp ph\u1ee7, ti\u00eau chu\u1ea9n ho\u00e0n thi\u1ec7n ngay tr\u00ean b\u1ea3n v\u1ebd \u0111\u1ec3 \u201c\u0111\u1eb9p \u0111\u00fang nh\u01b0 \u00fd\u201d.<\/p>\n<p>C\u1ea7n t\u01b0 v\u1ea5n m\u1eabu, th\u00f4ng s\u1ed1 ho\u00e0n thi\u1ec7n v\u00e0 b\u00e1o gi\u00e1 t\u1ed1t nh\u1ea5t cho d\u1ef1 \u00e1n t\u1ea1i H\u00e0 N\u1ed9i? Li\u00ean h\u1ec7 Inox C\u01b0\u1eddng Th\u1ecbnh \u2013 Hotline: 0343.417.281 \u2013 Email: inoxcongnghiep.cuongthinh@gmail.com<\/p>\n<p>Ngu\u1ed3n tham kh\u1ea3o:<br \/>\n&#8211; Nickel Institute \u2013 Finishing and Cleaning Stainless Steel; SSINA \u2013 Finishes (ASTM A480\/EN 10088).<br \/>\n&#8211; ISO 1302 (k\u00fd hi\u1ec7u nh\u00e1m b\u1ec1 m\u1eb7t), ISO 7599 (anod h\u00f3a nh\u00f4m).<br \/>\n&#8211; European Aluminium \u2013 Aluminium Finishing for Architecture.<br \/>\n&#8211; Copper Development Association \u2013 Copper, Brass and Bronze Architectural Finishes.<\/p>\n","protected":false},"excerpt":{"rendered":"<p>So s\u00e1nh chi ti\u1ebft v\u1ebb \u0111\u1eb9p v\u00e0 ho\u00e0n thi\u1ec7n b\u1ec1 m\u1eb7t c\u1ee7a Inox, \u0110\u1ed3ng, Nh\u00f4m: \u0111\u1ed9 b\u00f3ng, m\u00e0u s\u1eafc, b\u1ec1n m\u00e0u, ch\u1ed1ng v\u00e2n tay v\u00e0 \u1ee9ng d\u1ee5ng th\u1ef1c t\u1ebf cho n\u1ed9i ngo\u1ea1i th\u1ea5t.<\/p>\n","protected":false},"author":7,"featured_media":1002,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"_acf_changed":false,"footnotes":""},"categories":[23],"tags":[],"class_list":["post-1635","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-tin-tuc"],"acf":[],"_links":{"self":[{"href":"https:\/\/inoxcuongthinh.com\/inct\/wp\/v2\/posts\/1635","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/inoxcuongthinh.com\/inct\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/inoxcuongthinh.com\/inct\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/inoxcuongthinh.com\/inct\/wp\/v2\/users\/7"}],"replies":[{"embeddable":true,"href":"https:\/\/inoxcuongthinh.com\/inct\/wp\/v2\/comments?post=1635"}],"version-history":[{"count":0,"href":"https:\/\/inoxcuongthinh.com\/inct\/wp\/v2\/posts\/1635\/revisions"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/inoxcuongthinh.com\/inct\/wp\/v2\/media\/1002"}],"wp:attachment":[{"href":"https:\/\/inoxcuongthinh.com\/inct\/wp\/v2\/media?parent=1635"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/inoxcuongthinh.com\/inct\/wp\/v2\/categories?post=1635"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/inoxcuongthinh.com\/inct\/wp\/v2\/tags?post=1635"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}