{"id":2382,"date":"2026-08-01T11:03:26","date_gmt":"2026-08-01T04:03:26","guid":{"rendered":"https:\/\/inoxcuongthinh.com\/?post_type=product&#038;p=2382"},"modified":"2026-10-13T16:07:35","modified_gmt":"2026-10-13T09:07:35","slug":"tam-inox-304-0-35mm","status":"publish","type":"product","link":"https:\/\/inoxcuongthinh.com\/tam-inox-304-0-35mm\/","title":{"rendered":"T\u1ea5m Inox 304 0.35mm \u2013 Gi\u1ea3i ph\u00e1p v\u1eadt li\u1ec7u si\u00eau m\u1ecfng cho m\u1ecdi c\u00f4ng tr\u00ecnh"},"content":{"rendered":"<p class=\"ds-markdown-paragraph\"><span class=\"\">B\u1ea1n \u0111ang t\u00ecm ki\u1ebfm v\u1eadt li\u1ec7u inox m\u1ecfng nh\u1eb9 nh\u01b0ng b\u1ec1n b\u1ec9?\u00a0<\/span><strong><span class=\"\">T\u1ea5m inox 304 0.35mm<\/span><\/strong><span class=\"\">\u00a0ch\u00ednh l\u00e0 c\u00e2u tr\u1ea3 l\u1eddi ho\u00e0n h\u1ea3o. S\u1ea3n ph\u1ea9m n\u00e0y s\u1edf h\u1eefu \u0111\u1ed9 d\u00e0y si\u00eau m\u1ecfng ch\u1ec9 0.35mm. Nh\u1edd v\u1eady, n\u00f3 mang l\u1ea1i s\u1ef1 linh ho\u1ea1t t\u1ed1i \u0111a trong gia c\u00f4ng. V\u1eadt li\u1ec7u n\u00e0y \u0111\u00e1p \u1ee9ng t\u1ed1t c\u00e1c \u1ee9ng d\u1ee5ng \u0111\u00f2i h\u1ecfi t\u00ednh th\u1ea9m m\u1ef9 cao. B\u00e0i vi\u1ebft d\u01b0\u1edbi \u0111\u00e2y s\u1ebd cung c\u1ea5p m\u1ecdi th\u00f4ng tin c\u1ea7n thi\u1ebft v\u1ec1 s\u1ea3n ph\u1ea9m n\u00e0y.<\/span><\/p>\n<hr \/>\n<h2><span class=\"\">T\u1ed5ng quan v\u1ec1 t\u1ea5m inox 304 0.35mm<\/span><\/h2>\n<p class=\"ds-markdown-paragraph\"><strong><span class=\"\">T\u1ea5m inox 304 0.35mm<\/span><\/strong><span class=\"\">\u00a0l\u00e0 th\u00e9p kh\u00f4ng g\u1ec9 thu\u1ed9c nh\u00f3m Austenit. \u0110\u00e2y l\u00e0 d\u00f2ng th\u00e9p kh\u00f4ng g\u1ec9 ph\u1ed5 bi\u1ebfn nh\u1ea5t th\u1ebf gi\u1edbi<\/span><span class=\"\">. Th\u00e0nh ph\u1ea7n ch\u00ednh c\u1ee7a n\u00f3 g\u1ed3m 18% Crom v\u00e0 8% Niken<\/span><span class=\"\">. H\u00e0m l\u01b0\u1ee3ng n\u00e0y t\u1ea1o ra kh\u1ea3 n\u0103ng ch\u1ed1ng \u0103n m\u00f2n v\u01b0\u1ee3t tr\u1ed9i. \u0110\u1ed9 d\u00e0y 0.35mm thu\u1ed9c lo\u1ea1i si\u00eau m\u1ecfng, c\u1ef1c k\u1ef3 linh ho\u1ea1t. S\u1ea3n ph\u1ea9m \u0111\u01b0\u1ee3c s\u1ea3n xu\u1ea5t theo ti\u00eau chu\u1ea9n ASTM A240<\/span><span class=\"\">. Ti\u00eau chu\u1ea9n n\u00e0y \u0111\u1ea3m b\u1ea3o ch\u1ea5t l\u01b0\u1ee3ng \u1ed5n \u0111\u1ecbnh cho m\u1ecdi \u1ee9ng d\u1ee5ng. Nh\u1edd \u0111\u1ed9 d\u00e0y m\u1ecfng, v\u1eadt li\u1ec7u d\u1ec5 d\u00e0ng u\u1ed1n cong v\u00e0 t\u1ea1o h\u00ecnh<\/span><span class=\"\">.<\/span><\/p>\n<h3><span class=\"\">Th\u00e0nh ph\u1ea7n h\u00f3a h\u1ecdc c\u1ee7a inox 304<\/span><\/h3>\n<p class=\"ds-markdown-paragraph\"><span class=\"\">Ch\u1ea5t l\u01b0\u1ee3ng c\u1ee7a inox 304 \u0111\u1ebfn t\u1eeb th\u00e0nh ph\u1ea7n h\u00f3a h\u1ecdc \u0111\u1eb7c bi\u1ec7t. C\u00e1c nguy\u00ean t\u1ed1 h\u1ee3p kim \u0111\u00f3ng vai tr\u00f2 quan tr\u1ecdng. Crom t\u1ea1o ra l\u1edbp m\u00e0ng oxit b\u1ea3o v\u1ec7 b\u1ec1 m\u1eb7t<\/span><span class=\"\">. Niken gi\u00fap t\u0103ng \u0111\u1ed9 d\u1ebbo v\u00e0 kh\u1ea3 n\u0103ng ch\u1ecbu l\u1ef1c. B\u1ea3ng d\u01b0\u1edbi \u0111\u00e2y th\u1ec3 hi\u1ec7n th\u00e0nh ph\u1ea7n chi ti\u1ebft theo ti\u00eau chu\u1ea9n ASTM A240<\/span><span class=\"\">.<\/span><\/p>\n<div class=\"ds-scroll-area ds-scroll-area--show-on-focus-within ds-scroll-area--enabled _1210dd7 c03cafe9\">\n<div class=\"ds-scroll-area__gutters\">\n<div class=\"ds-scroll-area__horizontal-gutter\">\n<figure id=\"attachment_2383\" aria-describedby=\"caption-attachment-2383\" style=\"width: 679px\" class=\"wp-caption aligncenter\"><img decoding=\"async\" class=\"wp-image-2383\" src=\"https:\/\/inoxcuongthinh.com\/wp-content\/uploads\/2026\/08\/Tam-inox-304-0.35mm-300x240.png\" alt=\"T\u1ea5m inox 304 0.35mm\" width=\"679\" height=\"543\" title=\"\" srcset=\"https:\/\/inoxcuongthinh.com\/wp-content\/uploads\/2026\/08\/Tam-inox-304-0.35mm-300x240.png 300w, https:\/\/inoxcuongthinh.com\/wp-content\/uploads\/2026\/08\/Tam-inox-304-0.35mm-1024x819.png 1024w, https:\/\/inoxcuongthinh.com\/wp-content\/uploads\/2026\/08\/Tam-inox-304-0.35mm-768x615.png 768w, https:\/\/inoxcuongthinh.com\/wp-content\/uploads\/2026\/08\/Tam-inox-304-0.35mm-600x480.png 600w, https:\/\/inoxcuongthinh.com\/wp-content\/uploads\/2026\/08\/Tam-inox-304-0.35mm.png 1402w\" sizes=\"(max-width: 679px) 100vw, 679px\" \/><figcaption id=\"caption-attachment-2383\" class=\"wp-caption-text\">T\u1ea5m inox 304 0.35mm<\/figcaption><\/figure>\n<\/div>\n<div class=\"ds-scroll-area__vertical-gutter\"><\/div>\n<\/div>\n<table>\n<thead>\n<tr>\n<th><strong><span class=\"\">Nguy\u00ean t\u1ed1<\/span><\/strong><\/th>\n<th><strong><span class=\"\">K\u00fd hi\u1ec7u<\/span><\/strong><\/th>\n<th><strong><span class=\"\">H\u00e0m l\u01b0\u1ee3ng (%)<\/span><\/strong><\/th>\n<th><strong><span class=\"\">Vai tr\u00f2 ch\u00ednh<\/span><\/strong><\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td><span class=\"\">Crom<\/span><\/td>\n<td><span class=\"\">Cr<\/span><\/td>\n<td><span class=\"\">18.0 \u2013 20.0<\/span><\/td>\n<td><span class=\"\">T\u1ea1o kh\u1ea3 n\u0103ng ch\u1ed1ng \u0103n m\u00f2n<\/span><\/td>\n<\/tr>\n<tr>\n<td><span class=\"\">Niken<\/span><\/td>\n<td><span class=\"\">Ni<\/span><\/td>\n<td><span class=\"\">8.0 \u2013 10.5<\/span><\/td>\n<td><span class=\"\">T\u0103ng \u0111\u1ed9 d\u1ebbo v\u00e0 \u0111\u1ed9 b\u1ec1n dai<\/span><\/td>\n<\/tr>\n<tr>\n<td><span class=\"\">Cacbon<\/span><\/td>\n<td><span class=\"\">C<\/span><\/td>\n<td><span class=\"\">\u2264 0.08<\/span><\/td>\n<td><span class=\"\">T\u0103ng \u0111\u1ed9 c\u1ee9ng cho v\u1eadt li\u1ec7u<\/span><\/td>\n<\/tr>\n<tr>\n<td><span class=\"\">Mangan<\/span><\/td>\n<td><span class=\"\">Mn<\/span><\/td>\n<td><span class=\"\">\u2264 2.0<\/span><\/td>\n<td><span class=\"\">\u1ed4n \u0111\u1ecbnh c\u1ea5u tr\u00fac trong s\u1ea3n xu\u1ea5t<\/span><\/td>\n<\/tr>\n<tr>\n<td><span class=\"\">Silicon<\/span><\/td>\n<td><span class=\"\">Si<\/span><\/td>\n<td><span class=\"\">\u2264 0.75<\/span><\/td>\n<td><span class=\"\">T\u0103ng kh\u1ea3 n\u0103ng ch\u1ed1ng oxy h\u00f3a<\/span><\/td>\n<\/tr>\n<tr>\n<td><span class=\"\">Ph\u1ed1t pho<\/span><\/td>\n<td><span class=\"\">P<\/span><\/td>\n<td><span class=\"\">\u2264 0.045<\/span><\/td>\n<td><span class=\"\">T\u1ea1p ch\u1ea5t, duy tr\u00ec \u1edf m\u1ee9c th\u1ea5p<\/span><\/td>\n<\/tr>\n<tr>\n<td><span class=\"\">L\u01b0u hu\u1ef3nh<\/span><\/td>\n<td><span class=\"\">S<\/span><\/td>\n<td><span class=\"\">\u2264 0.030<\/span><\/td>\n<td><span class=\"\">T\u1ea1p ch\u1ea5t, duy tr\u00ec \u1edf m\u1ee9c th\u1ea5p<\/span><\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<\/div>\n<p class=\"ds-markdown-paragraph\"><span class=\"\">H\u00e0m l\u01b0\u1ee3ng cacbon th\u1ea5p gi\u00fap inox d\u1ec5 h\u00e0n h\u01a1n. \u0110i\u1ec1u n\u00e0y r\u1ea5t quan tr\u1ecdng v\u1edbi c\u00e1c chi ti\u1ebft nh\u1ecf. Inox 304L c\u00f3 l\u01b0\u1ee3ng cacbon th\u1ea5p h\u01a1n (\u2264 0.03%)<\/span><span class=\"\">. Phi\u00ean b\u1ea3n n\u00e0y tr\u00e1nh \u0111\u01b0\u1ee3c \u0103n m\u00f2n li\u00ean h\u1ea1t sau h\u00e0n.<\/span><\/p>\n<h3><span class=\"\">Th\u00f4ng s\u1ed1 v\u1eadt l\u00fd quan tr\u1ecdng<\/span><\/h3>\n<p class=\"ds-markdown-paragraph\"><span class=\"\">Hi\u1ec3u r\u00f5 th\u00f4ng s\u1ed1 v\u1eadt l\u00fd gi\u00fap b\u1ea1n s\u1eed d\u1ee5ng inox hi\u1ec7u qu\u1ea3. B\u1ea3ng d\u01b0\u1edbi \u0111\u00e2y t\u1ed5ng h\u1ee3p c\u00e1c t\u00ednh ch\u1ea5t quan tr\u1ecdng<\/span><span class=\"\">.<\/span><\/p>\n<div class=\"ds-scroll-area ds-scroll-area--show-on-focus-within ds-scroll-area--enabled _1210dd7 c03cafe9\">\n<div class=\"ds-scroll-area__gutters\">\n<div class=\"ds-scroll-area__horizontal-gutter\"><\/div>\n<div class=\"ds-scroll-area__vertical-gutter\"><\/div>\n<\/div>\n<table>\n<thead>\n<tr>\n<th><strong><span class=\"\">T\u00ednh ch\u1ea5t<\/span><\/strong><\/th>\n<th><strong><span class=\"\">Gi\u00e1 tr\u1ecb<\/span><\/strong><\/th>\n<th><strong><span class=\"\">\u00dd ngh\u0129a<\/span><\/strong><\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td><span class=\"\">Kh\u1ed1i l\u01b0\u1ee3ng ri\u00eang<\/span><\/td>\n<td><span class=\"\">7.93 g\/cm\u00b3<\/span><\/td>\n<td><span class=\"\">X\u00e1c \u0111\u1ecbnh tr\u1ecdng l\u01b0\u1ee3ng c\u1ee7a t\u1ea5m inox<\/span><\/td>\n<\/tr>\n<tr>\n<td><span class=\"\">Nhi\u1ec7t \u0111\u1ed9 n\u00f3ng ch\u1ea3y<\/span><\/td>\n<td><span class=\"\">1400 \u2013 1450 \u00b0C<\/span><\/td>\n<td><span class=\"\">Kh\u1ea3 n\u0103ng ch\u1ecbu nhi\u1ec7t \u1edf m\u1ee9c r\u1ea5t cao<\/span><\/td>\n<\/tr>\n<tr>\n<td><span class=\"\">Gi\u1edbi h\u1ea1n b\u1ec1n k\u00e9o<\/span><\/td>\n<td><span class=\"\">\u2265 515 MPa<\/span><\/td>\n<td><span class=\"\">Kh\u1ea3 n\u0103ng ch\u1ecbu l\u1ef1c k\u00e9o t\u1ed1i \u0111a<\/span><\/td>\n<\/tr>\n<tr>\n<td><span class=\"\">Gi\u1edbi h\u1ea1n ch\u1ea3y<\/span><\/td>\n<td><span class=\"\">\u2265 205 MPa<\/span><\/td>\n<td><span class=\"\">Kh\u1ea3 n\u0103ng ch\u1ecbu l\u1ef1c tr\u01b0\u1edbc khi bi\u1ebfn d\u1ea1ng<\/span><\/td>\n<\/tr>\n<tr>\n<td><span class=\"\">\u0110\u1ed9 gi\u00e3n d\u00e0i<\/span><\/td>\n<td><span class=\"\">\u2265 40%<\/span><\/td>\n<td><span class=\"\">\u0110\u1ed9 d\u1ebbo v\u00e0 kh\u1ea3 n\u0103ng bi\u1ebfn d\u1ea1ng<\/span><\/td>\n<\/tr>\n<tr>\n<td><span class=\"\">\u0110\u1ed9 c\u1ee9ng Rockwell<\/span><\/td>\n<td><span class=\"\">\u2264 92 HRB<\/span><\/td>\n<td><span class=\"\">\u0110\u1ed9 c\u1ee9ng b\u1ec1 m\u1eb7t c\u1ee7a v\u1eadt li\u1ec7u<\/span><\/td>\n<\/tr>\n<tr>\n<td><span class=\"\">\u0110\u1ed9 d\u1eabn nhi\u1ec7t<\/span><\/td>\n<td><span class=\"\">16.2 W\/m.K<\/span><\/td>\n<td><span class=\"\">Truy\u1ec1n nhi\u1ec7t \u1edf m\u1ee9c trung b\u00ecnh<\/span><\/td>\n<\/tr>\n<tr>\n<td><span class=\"\">\u0110i\u1ec7n tr\u1edf su\u1ea5t<\/span><\/td>\n<td><span class=\"\">0.72 \u03bc\u03a9.m<\/span><\/td>\n<td><span class=\"\">T\u00ednh ch\u1ea5t c\u00e1ch \u0111i\u1ec7n t\u01b0\u01a1ng \u0111\u1ed1i<\/span><\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<\/div>\n<p class=\"ds-markdown-paragraph\"><span class=\"\">Inox 304 c\u00f3 kh\u1ea3 n\u0103ng ch\u1ecbu oxy h\u00f3a \u1edf nhi\u1ec7t \u0111\u1ed9 870-925\u00b0C<\/span><span class=\"\">. V\u1eadt li\u1ec7u h\u1ea7u nh\u01b0 kh\u00f4ng c\u00f3 t\u01b0\u01a1ng t\u00e1c t\u1eeb t\u00ednh<\/span><span class=\"\">. \u0110i\u1ec1u n\u00e0y r\u1ea5t h\u1eefu \u00edch trong c\u00e1c \u1ee9ng d\u1ee5ng \u0111i\u1ec7n t\u1eed. Kh\u1ed1i l\u01b0\u1ee3ng ri\u00eang 7.93 g\/cm\u00b3 gi\u00fap b\u1ea1n d\u1ec5 d\u00e0ng t\u00ednh tr\u1ecdng l\u01b0\u1ee3ng.<\/span><\/p>\n<hr \/>\n<h2><span class=\"\">Nh\u1eefng \u01b0u \u0111i\u1ec3m v\u01b0\u1ee3t tr\u1ed9i c\u1ee7a s\u1ea3n ph\u1ea9m<\/span><\/h2>\n<p class=\"ds-markdown-paragraph\"><strong><span class=\"\">T\u1ea5m inox 304 0.35mm<\/span><\/strong><span class=\"\">\u00a0s\u1edf h\u1eefu nhi\u1ec1u \u01b0u \u0111i\u1ec3m n\u1ed5i b\u1eadt:<\/span><\/p>\n<ul>\n<li>\n<p class=\"ds-markdown-paragraph\"><strong><span class=\"\">Ch\u1ed1ng \u0103n m\u00f2n v\u00e0 g\u1ec9 s\u00e9t tuy\u1ec7t v\u1eddi:<\/span><\/strong><span class=\"\">\u00a0Crom v\u00e0 niken t\u1ea1o l\u1edbp m\u00e0ng th\u1ee5 \u0111\u1ed9ng b\u1ea3o v\u1ec7. V\u1eadt li\u1ec7u ch\u1ed1ng l\u1ea1i h\u00f3a ch\u1ea5t v\u00e0 m\u00f4i tr\u01b0\u1eddng \u1ea9m \u01b0\u1edbt<\/span><span class=\"\">.<\/span><\/p>\n<\/li>\n<li>\n<p class=\"ds-markdown-paragraph\"><strong><span class=\"\">\u0110\u1ed9 b\u1ec1n c\u01a1 h\u1ecdc cao:<\/span><\/strong><span class=\"\">\u00a0Gi\u1edbi h\u1ea1n b\u1ec1n k\u00e9o \u0111\u1ea1t 515 MPa. V\u1eadt li\u1ec7u ch\u1ecbu \u0111\u01b0\u1ee3c va \u0111\u1eadp v\u00e0 \u00e1p l\u1ef1c t\u1ed1t<\/span><span class=\"\">.<\/span><\/p>\n<\/li>\n<li>\n<p class=\"ds-markdown-paragraph\"><strong><span class=\"\">Si\u00eau m\u1ecfng v\u00e0 linh ho\u1ea1t:<\/span><\/strong><span class=\"\">\u00a0\u0110\u1ed9 d\u00e0y 0.35mm cho ph\u00e9p u\u1ed1n cong d\u1ec5 d\u00e0ng. B\u1ea1n c\u00f3 th\u1ec3 t\u1ea1o ra c\u00e1c s\u1ea3n ph\u1ea9m ph\u1ee9c t\u1ea1p<\/span><span class=\"\">.<\/span><\/p>\n<\/li>\n<li>\n<p class=\"ds-markdown-paragraph\"><strong><span class=\"\">T\u00ednh th\u1ea9m m\u1ef9 v\u00e0 v\u1ec7 sinh cao:<\/span><\/strong><span class=\"\">\u00a0B\u1ec1 m\u1eb7t s\u00e1ng b\u00f3ng, d\u1ec5 lau ch\u00f9i. V\u1eadt li\u1ec7u lu\u00f4n gi\u1eef \u0111\u01b0\u1ee3c v\u1ebb \u0111\u1eb9p theo th\u1eddi gian.<\/span><\/p>\n<\/li>\n<li>\n<p class=\"ds-markdown-paragraph\"><strong><span class=\"\">An to\u00e0n tuy\u1ec7t \u0111\u1ed1i v\u1edbi s\u1ee9c kh\u1ecfe:<\/span><\/strong><span class=\"\">\u00a0Inox 304 kh\u00f4ng ch\u1ee9a ch\u1ea5t \u0111\u1ed9c h\u1ea1i. S\u1ea3n ph\u1ea9m \u0111\u01b0\u1ee3c d\u00f9ng r\u1ed9ng r\u00e3i trong th\u1ef1c ph\u1ea9m v\u00e0 y t\u1ebf<\/span><span class=\"\">.<\/span><\/p>\n<\/li>\n<li>\n<p class=\"ds-markdown-paragraph\"><strong><span class=\"\">D\u1ec5 d\u00e0ng gia c\u00f4ng:<\/span><\/strong><span class=\"\">\u00a0Inox 304 c\u00f3 kh\u1ea3 n\u0103ng t\u1ea1o h\u00ecnh v\u00e0 h\u00e0n t\u1ed1t<\/span><span class=\"\">. Kh\u00f4ng c\u1ea7n x\u1eed l\u00fd nhi\u1ec7t sau khi gia c\u00f4ng<\/span><span class=\"\">.<\/span><\/p>\n<\/li>\n<\/ul>\n<hr \/>\n<h2><span class=\"\">\u1ee8ng d\u1ee5ng \u0111a d\u1ea1ng trong \u0111\u1eddi s\u1ed1ng<\/span><\/h2>\n<p class=\"ds-markdown-paragraph\"><span class=\"\">\u0110\u1ed9 d\u00e0y si\u00eau m\u1ecfng 0.35mm m\u1edf ra nhi\u1ec1u \u1ee9ng d\u1ee5ng th\u00fa v\u1ecb.<\/span><\/p>\n<h3><span class=\"\">Trong \u0111\u1eddi s\u1ed1ng v\u00e0 n\u1ed9i th\u1ea5t<\/span><\/h3>\n<p class=\"ds-markdown-paragraph\"><span class=\"\">B\u1ea1n s\u1ebd b\u1eaft g\u1eb7p\u00a0<\/span><strong><span class=\"\">t\u1ea5m inox 304 0.35mm<\/span><\/strong><span class=\"\">\u00a0trong nhi\u1ec1u v\u1eadt d\u1ee5ng quen thu\u1ed9c. Ng\u01b0\u1eddi ta d\u00f9ng n\u00f3 \u0111\u1ec3 s\u1ea3n xu\u1ea5t m\u1eb7t b\u00e0n b\u1ebfp, t\u1ee7 l\u1ea1nh<\/span><span class=\"\">. N\u00f3 c\u00f2n \u0111\u01b0\u1ee3c d\u00f9ng l\u00e0m v\u00e1ch ng\u0103n trang tr\u00ed v\u00e0 lan can c\u1ea7u thang. V\u1ebb ngo\u00e0i s\u00e1ng b\u00f3ng gi\u00fap kh\u00f4ng gian s\u1ed1ng th\u00eam sang tr\u1ecdng.<\/span><\/p>\n<h3><span class=\"\">Trong c\u00f4ng nghi\u1ec7p v\u00e0 s\u1ea3n xu\u1ea5t<\/span><\/h3>\n<p class=\"ds-markdown-paragraph\"><span class=\"\">Ng\u00e0nh c\u00f4ng nghi\u1ec7p ch\u1ebf bi\u1ebfn th\u1ef1c ph\u1ea9m r\u1ea5t \u01b0a chu\u1ed9ng lo\u1ea1i inox n\u00e0y. C\u00e1c thi\u1ebft b\u1ecb nh\u01b0 b\u1ed3n ch\u1ee9a, \u1ed1ng d\u1eabn \u0111\u1ec1u c\u1ea7n \u0111\u1ebfn n\u00f3<\/span><span class=\"\">. Trong c\u00f4ng nghi\u1ec7p h\u00f3a ch\u1ea5t, n\u00f3 d\u00f9ng l\u00e0m th\u00f9ng ch\u1ee9a dung m\u00f4i<\/span><span class=\"\">. Ng\u00e0nh d\u01b0\u1ee3c ph\u1ea9m v\u00e0 m\u1ef9 ph\u1ea9m c\u0169ng s\u1eed d\u1ee5ng v\u00ec t\u00ednh v\u00f4 tr\u00f9ng. Ngo\u00e0i ra, n\u00f3 c\u00f2n d\u00f9ng l\u00e0m l\u01b0\u1edbi l\u1ecdc v\u00e0 chi ti\u1ebft m\u00e1y m\u00f3c.<\/span><\/p>\n<h3><span class=\"\">Trong c\u00e1c \u1ee9ng d\u1ee5ng k\u1ef9 thu\u1eadt \u0111\u1eb7c bi\u1ec7t<\/span><\/h3>\n<p class=\"ds-markdown-paragraph\"><span class=\"\">\u0110\u1ed9 d\u00e0y 0.35mm r\u1ea5t ph\u00f9 h\u1ee3p cho c\u00e1c \u1ee9ng d\u1ee5ng k\u1ef9 thu\u1eadt nh\u1eb9<\/span><span class=\"\">. S\u1ea3n ph\u1ea9m d\u00f9ng l\u00e0m shim ch\u00eam, l\u00e1 c\u0103n trong l\u1eafp r\u00e1p m\u00e1y m\u00f3c<\/span><span class=\"\">. N\u00f3 c\u0169ng \u0111\u01b0\u1ee3c s\u1eed d\u1ee5ng trong ng\u00e0nh h\u00e0ng kh\u00f4ng v\u00e0 \u0111i\u1ec7n t\u1eed. \u0110\u1ed9 m\u1ecfng gi\u00fap ti\u1ebft ki\u1ec7m kh\u00f4ng gian v\u00e0 tr\u1ecdng l\u01b0\u1ee3ng.<\/span><\/p>\n<hr \/>\n<h2><span class=\"\">Quy c\u00e1ch v\u00e0 b\u1ec1 m\u1eb7t ph\u1ed5 bi\u1ebfn<\/span><\/h2>\n<p class=\"ds-markdown-paragraph\"><span class=\"\">Kh\u00e1ch h\u00e0ng c\u00f3 nhi\u1ec1u l\u1ef1a ch\u1ecdn v\u1ec1 k\u00edch th\u01b0\u1edbc v\u00e0 b\u1ec1 m\u1eb7t<\/span><span class=\"\">:<\/span><\/p>\n<ul>\n<li>\n<p class=\"ds-markdown-paragraph\"><strong><span class=\"\">Kh\u1ed5 r\u1ed9ng ph\u1ed5 bi\u1ebfn:<\/span><\/strong><span class=\"\">\u00a0800mm, 1000mm, 1200mm, 1240mm.<\/span><\/p>\n<\/li>\n<li>\n<p class=\"ds-markdown-paragraph\"><strong><span class=\"\">Chi\u1ec1u d\u00e0i:<\/span><\/strong><span class=\"\">\u00a01m, 2m, 2.5m, 3m, 6m ho\u1eb7c theo y\u00eau c\u1ea7u.<\/span><\/p>\n<\/li>\n<li>\n<p class=\"ds-markdown-paragraph\"><strong><span class=\"\">B\u1ec1 m\u1eb7t \u0111a d\u1ea1ng:<\/span><\/strong><span class=\"\">\u00a0BA (b\u00f3ng g\u01b0\u01a1ng), 2B (m\u1edd ti\u00eau chu\u1ea9n), No.4 (x\u01b0\u1edbc), HL (x\u01b0\u1edbc d\u00e0i), g\u00e2n nh\u00e1m, v\u00e2n ca r\u00f4<\/span><span class=\"\">.<\/span><\/p>\n<\/li>\n<\/ul>\n<hr \/>\n<h2><a href=\"https:\/\/inoxcuongthinh.com\/bang-bao-gia-tam-inox-304-do-day\/\"><span class=\"\">Mua t\u1ea5m inox 304 0.35mm ch\u1ea5t l\u01b0\u1ee3ng<\/span><\/a><\/h2>\n<p class=\"ds-markdown-paragraph\"><span class=\"\">\u0110\u1ec3 \u0111\u01b0\u1ee3c t\u01b0 v\u1ea5n v\u00e0 nh\u1eadn b\u00e1o gi\u00e1 t\u1ed1t nh\u1ea5t, h\u00e3y li\u00ean h\u1ec7 ngay v\u1edbi ch\u00fang t\u00f4i. C\u00f4ng ty TNHH INOX C\u00f4ng Nghi\u1ec7p C\u01b0\u1eddng Th\u1ecbnh l\u00e0 \u0111\u01a1n v\u1ecb uy t\u00edn h\u00e0ng \u0111\u1ea7u. Ch\u00fang t\u00f4i chuy\u00ean cung c\u1ea5p c\u00e1c s\u1ea3n ph\u1ea9m inox nh\u1eadp kh\u1ea9u ch\u00ednh h\u00e3ng. H\u00e0ng h\u00f3a c\u00f3 \u0111\u1ea7y \u0111\u1ee7 ch\u1ee9ng ch\u1ec9 CO, CQ. S\u1ea3n ph\u1ea9m \u0111a d\u1ea1ng v\u1ec1 quy c\u00e1ch v\u00e0 b\u1ec1 m\u1eb7t. Ch\u00fang t\u00f4i h\u1ed7 tr\u1ee3 gia c\u00f4ng c\u1eaft, x\u1ebb b\u0103ng theo y\u00eau c\u1ea7u. Ch\u00ednh s\u00e1ch v\u1eadn chuy\u1ec3n linh ho\u1ea1t cho m\u1ecdi \u0111\u01a1n h\u00e0ng.<\/span><\/p>\n<p class=\"ds-markdown-paragraph\"><span class=\"\">Li\u00ean h\u1ec7 ngay h\u00f4m nay \u0111\u1ec3 nh\u1eadn \u01b0u \u0111\u00e3i:<\/span><\/p>\n<ul>\n<li>\n<p class=\"ds-markdown-paragraph\"><strong><span class=\"\">WEBSITE:<\/span><\/strong><span class=\"\">\u00a0<\/span><a href=\"https:\/\/inoxcuongthinh.com\/\" target=\"_blank\" rel=\"noopener noreferrer\"><span class=\"\">https:\/\/inoxcuongthinh.com\/<\/span><\/a><\/p>\n<\/li>\n<li>\n<p class=\"ds-markdown-paragraph\"><strong><span class=\"\">Hotline:<\/span><\/strong><span class=\"\">\u00a00343.417.281 \u2013 0904.274.898<\/span><\/p>\n<\/li>\n<li>\n<p class=\"ds-markdown-paragraph\"><strong><span class=\"\">\u0110\u1ecba Ch\u1ec9:<\/span><\/strong><span class=\"\">\u00a0\u0110\u1ed9i 6 th\u00f4n V\u0129nh Trung, x\u00e3 Ng\u1ecdc H\u1ed3i, th\u00e0nh ph\u1ed1 H\u00e0 N\u1ed9i, Vi\u1ec7t Nam.<\/span><\/p>\n<\/li>\n<\/ul>\n<p><a href=\"https:\/\/inoxcuongthinh.com\/lien-he\/\"><img decoding=\"async\" class=\"wp-image-2318 aligncenter\" src=\"https:\/\/inoxcuongthinh.com\/wp-content\/uploads\/2026\/07\/lien-he-300x176.png\" alt=\"\" width=\"753\" height=\"442\" title=\"\" srcset=\"https:\/\/inoxcuongthinh.com\/wp-content\/uploads\/2026\/07\/lien-he-300x176.png 300w, https:\/\/inoxcuongthinh.com\/wp-content\/uploads\/2026\/07\/lien-he-1024x600.png 1024w, https:\/\/inoxcuongthinh.com\/wp-content\/uploads\/2026\/07\/lien-he-768x450.png 768w, https:\/\/inoxcuongthinh.com\/wp-content\/uploads\/2026\/07\/lien-he-600x352.png 600w, https:\/\/inoxcuongthinh.com\/wp-content\/uploads\/2026\/07\/lien-he.png 1525w\" sizes=\"(max-width: 753px) 100vw, 753px\" \/><\/a><\/p>\n","protected":false},"excerpt":{"rendered":"<p>T\u00ecm hi\u1ec3u v\u1ec1 t\u1ea5m inox 304 0.35mm: th\u00e0nh ph\u1ea7n, \u01b0u \u0111i\u1ec3m, \u1ee9ng d\u1ee5ng v\u00e0 b\u00e1o gi\u00e1 chi ti\u1ebft. Li\u00ean h\u1ec7 C\u01b0\u1eddng Th\u1ecbnh \u0111\u1ec3 mua t\u1ea5m inox 304 0.35mm gi\u00e1 t\u1ed1t nh\u1ea5t.<\/p>\n","protected":false},"featured_media":2383,"comment_status":"open","ping_status":"closed","template":"","meta":{"_acf_changed":false},"product_brand":[],"product_cat":[53],"product_tag":[],"class_list":["post-2382","product","type-product","status-publish","has-post-thumbnail","product_cat-inox","first","instock","sale","shipping-taxable","purchasable","product-type-simple"],"acf":[],"_links":{"self":[{"href":"https:\/\/inoxcuongthinh.com\/inct\/wp\/v2\/product\/2382","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/inoxcuongthinh.com\/inct\/wp\/v2\/product"}],"about":[{"href":"https:\/\/inoxcuongthinh.com\/inct\/wp\/v2\/types\/product"}],"replies":[{"embeddable":true,"href":"https:\/\/inoxcuongthinh.com\/inct\/wp\/v2\/comments?post=2382"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/inoxcuongthinh.com\/inct\/wp\/v2\/media\/2383"}],"wp:attachment":[{"href":"https:\/\/inoxcuongthinh.com\/inct\/wp\/v2\/media?parent=2382"}],"wp:term":[{"taxonomy":"product_brand","embeddable":true,"href":"https:\/\/inoxcuongthinh.com\/inct\/wp\/v2\/product_brand?post=2382"},{"taxonomy":"product_cat","embeddable":true,"href":"https:\/\/inoxcuongthinh.com\/inct\/wp\/v2\/product_cat?post=2382"},{"taxonomy":"product_tag","embeddable":true,"href":"https:\/\/inoxcuongthinh.com\/inct\/wp\/v2\/product_tag?post=2382"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}