{"id":957,"date":"2025-09-21T21:21:05","date_gmt":"2025-09-21T14:21:05","guid":{"rendered":"https:\/\/inoxcuongthinh.com\/san-pham\/day-inox-201\/"},"modified":"2025-11-11T09:50:13","modified_gmt":"2025-11-11T02:50:13","slug":"day-inox-201","status":"publish","type":"product","link":"https:\/\/inoxcuongthinh.com\/day-inox-201\/","title":{"rendered":"D\u00e2y inox 201"},"content":{"rendered":"<h3>T\u1ed5ng quan v\u1ec1 D\u00e2y inox 201<\/h3>\n<p>D\u00e2y inox 201 (th\u00e9p kh\u00f4ng g\u1ec9 201) l\u00e0 d\u1ea1ng d\u00e2y tr\u00f2n k\u00e9o ngu\u1ed9i t\u1eeb m\u00e1c th\u00e9p austenitic 201, c\u00f2n \u0111\u01b0\u1ee3c bi\u1ebft \u0111\u1ebfn v\u1edbi c\u00e1c t\u00ean g\u1ecdi AISI 201, SUS201 (JIS), EN 1.4372. Nh\u1edd h\u00e0m l\u01b0\u1ee3ng Ni th\u1ea5p v\u00e0 Mn cao, inox 201 c\u00f3 gi\u00e1 th\u00e0nh c\u1ea1nh tranh nh\u01b0ng v\u1eabn gi\u1eef \u0111\u01b0\u1ee3c b\u1ec1 m\u1eb7t s\u00e1ng, kh\u1ea3 n\u0103ng t\u1ea1o h\u00ecnh v\u00e0 \u0111\u1ed9 b\u1ec1n c\u01a1 h\u1ecdc t\u1ed1t. Tr\u00ean th\u1ecb tr\u01b0\u1eddng, d\u00e2y inox 201 l\u00e0 l\u1ef1a ch\u1ecdn ph\u1ed5 bi\u1ebfn cho c\u00e1c \u1ee9ng d\u1ee5ng trong nh\u00e0, m\u00f4i tr\u01b0\u1eddng kh\u00f4\/\u00edt \u0103n m\u00f2n, s\u1ea3n xu\u1ea5t \u0111\u1ed3 gia d\u1ee5ng \u2013 trang tr\u00ed, l\u01b0\u1edbi \u2013 k\u1ec7 \u2013 m\u00f3c treo v\u00e0 c\u00e1c chi ti\u1ebft c\u01a1 kh\u00ed nh\u1eb9 \u0111\u00f2i h\u1ecfi t\u00ednh th\u1ea9m m\u1ef9 v\u00e0 \u0111\u1ed9 c\u1ee9ng v\u1eefng.<\/p>\n<h3>B\u1ea3ng th\u00f4ng s\u1ed1 k\u1ef9 thu\u1eadt chi ti\u1ebft<\/h3>\n<table>\n<tbody>\n<tr>\n<td><strong>M\u00e1c th\u00e9p<\/strong><\/td>\n<td>AISI 201; SUS201 (JIS); EN 1.4372<\/td>\n<\/tr>\n<tr>\n<td><strong>Ti\u00eau chu\u1ea9n<\/strong><\/td>\n<td>ASTM A580\/A580M (stainless steel wire); EN 10088; AISI\/SAE; JIS (SUS201)<\/td>\n<\/tr>\n<tr>\n<td><strong>Th\u00e0nh ph\u1ea7n h\u00f3a h\u1ecdc (%)<\/strong><\/td>\n<td>C \u2264 0,15; Mn 5,5\u20137,5; Cr 16,0\u201318,0; Ni 3,5\u20135,5; Si \u2264 1,0; N \u2264 0,25; P \u2264 0,060; S \u2264 0,030 (tham chi\u1ebfu m\u00e1c 201)<\/td>\n<\/tr>\n<tr>\n<td><strong>T\u00ednh ch\u1ea5t c\u01a1 l\u00fd<\/strong><\/td>\n<td>\u0110\u1ed9 b\u1ec1n k\u00e9o Rm (\u1ee7 m\u1ec1m) \u2265 515 MPa; Gi\u1edbi h\u1ea1n ch\u1ea3y Rp0,2 \u2265 275 MPa; \u0110\u1ed9 d\u00e3n d\u00e0i A50 \u2265 40%; \u0110\u1ed9 c\u1ee9ng \u1ee7 m\u1ec1m \u2264 95 HRB; Kh\u1ed1i l\u01b0\u1ee3ng ri\u00eang ~7,93 g\/cm\u00b3; T\u1eeb t\u00ednh: r\u1ea5t th\u1ea5p \u0111\u1ebfn h\u01a1i nhi\u1ec5m t\u1eeb sau c\u00e1n\/k\u00e9o ngu\u1ed9i<\/td>\n<\/tr>\n<tr>\n<td><strong>\u0110\u1ed9 d\u00e0y ph\u1ed5 bi\u1ebfn<\/strong><\/td>\n<td>\u0110\u01b0\u1eddng k\u00ednh d\u00e2y: 0,30\u201310,0 mm (\u0111\u1eb7t h\u00e0ng theo y\u00eau c\u1ea7u c\u00f3 th\u1ec3 t\u1edbi 12\u201314 mm t\u00f9y l\u00f4)<\/td>\n<\/tr>\n<tr>\n<td><strong>K\u00edch th\u01b0\u1edbc ti\u00eau chu\u1ea9n<\/strong><\/td>\n<td>D\u1ea1ng cu\u1ed9n: 10\u2013500 kg\/cu\u1ed9n; \u0110\u01b0\u1eddng k\u00ednh trong cu\u1ed9n (ID): ~200\u2013400 mm; Dung sai \u0111\u01b0\u1eddng k\u00ednh tham chi\u1ebfu ASTM A580: \u00b10,02\u20130,05 mm t\u00f9y c\u1ee1<\/td>\n<\/tr>\n<tr>\n<td><strong>B\u1ec1 m\u1eb7t<\/strong><\/td>\n<td>Bright-drawn (s\u00e1ng b\u00f3ng), \u1ee7 m\u1ec1m\/bright-annealed (BA), b\u1ec1 m\u1eb7t nh\u1eb5n, c\u00f3 th\u1ec3 ph\u1ee7 d\u1ea7u ch\u1ed1ng g\u1ec9 b\u1ea3o qu\u1ea3n<\/td>\n<\/tr>\n<tr>\n<td><strong>Xu\u1ea5t x\u1ee9<\/strong><\/td>\n<td>Vi\u1ec7t Nam\/Trung Qu\u1ed1c\/\u1ea4n \u0110\u1ed9\/\u0110\u00e0i Loan; Cung c\u1ea5p k\u00e8m CO\/CQ theo l\u00f4 h\u00e0ng<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<p>L\u01b0u \u00fd: Gi\u00e1 tr\u1ecb c\u01a1 l\u00fd v\u00e0 dung sai c\u00f3 th\u1ec3 thay \u0111\u1ed5i theo tr\u1ea1ng th\u00e1i nhi\u1ec7t luy\u1ec7n (\u1ee7 m\u1ec1m\/c\u00e1n ngu\u1ed9i), c\u1ee1 d\u00e2y v\u00e0 t\u1eebng ti\u00eau chu\u1ea9n\/l\u00f4 s\u1ea3n xu\u1ea5t. Inox C\u01b0\u1eddng Th\u1ecbnh cung c\u1ea5p ki\u1ec3m \u0111\u1ecbnh k\u00e8m h\u1ed3 s\u01a1 CO\/CQ theo y\u00eau c\u1ea7u.<\/p>\n<h3>So s\u00e1nh D\u00e2y inox 201 v\u1edbi c\u00e1c lo\u1ea1i ph\u1ed5 bi\u1ebfn kh\u00e1c<\/h3>\n<p>&#8211; So v\u1edbi inox 304:<br \/>\n  &#8211; Kh\u1ea3 n\u0103ng ch\u1ed1ng \u0103n m\u00f2n: 201 th\u1ea5p h\u01a1n 304 do h\u00e0m l\u01b0\u1ee3ng Ni th\u1ea5p; 304 ph\u00f9 h\u1ee3p m\u00f4i tr\u01b0\u1eddng ngo\u00e0i tr\u1eddi, \u1ea9m, c\u00f3 clorua; 201 n\u00ean \u01b0u ti\u00ean m\u00f4i tr\u01b0\u1eddng kh\u00f4\/\u00edt \u0103n m\u00f2n.<br \/>\n  &#8211; Gi\u00e1 th\u00e0nh: 201 th\u01b0\u1eddng r\u1ebb h\u01a1n 304 \u0111\u00e1ng k\u1ec3, t\u1ed1i \u01b0u chi ph\u00ed cho c\u00e1c \u1ee9ng d\u1ee5ng kh\u00f4ng qu\u00e1 kh\u1eaft khe v\u1ec1 \u0103n m\u00f2n.<br \/>\n  &#8211; Gia c\u00f4ng: C\u1ea3 hai \u0111\u1ec1u d\u1ec5 u\u1ed1n \u2013 k\u00e9o \u2013 h\u00e0n; 201 c\u1ee9ng h\u01a1n \u0111\u00f4i ch\u00fat khi c\u00e1n\/k\u00e9o ngu\u1ed9i v\u00e0 c\u00f3 th\u1ec3 h\u01a1i nhi\u1ec5m t\u1eeb; 304 h\u1ea7u nh\u01b0 kh\u00f4ng nhi\u1ec5m t\u1eeb \u1edf tr\u1ea1ng th\u00e1i \u1ee7 m\u1ec1m.<br \/>\n  &#8211; \u1ee8ng d\u1ee5ng: 201 ph\u00f9 h\u1ee3p \u0111\u1ed3 gia d\u1ee5ng, n\u1ed9i th\u1ea5t, l\u01b0\u1edbi \u2013 gi\u00e1 k\u1ec7, chi ti\u1ebft trang tr\u00ed trong nh\u00e0; 304 d\u00f9ng cho th\u1ef1c ph\u1ea9m, y t\u1ebf, h\u00f3a ch\u1ea5t nh\u1eb9 v\u00e0 ngo\u00e0i tr\u1eddi.<\/p>\n<h3>\u1ee8ng d\u1ee5ng th\u1ef1c t\u1ebf c\u1ee7a D\u00e2y inox 201<\/h3>\n<p>&#8211; Trong gia d\u1ee5ng \u2013 n\u1ed9i th\u1ea5t: m\u00f3c treo, k\u1ec7 \u2013 r\u1ed5 \u2013 khung, gi\u00e0n ph\u01a1i, ph\u1ee5 ki\u1ec7n trang tr\u00ed.<br \/>\n&#8211; Trong x\u00e2y d\u1ef1ng \u2013 qu\u1ea3ng c\u00e1o: d\u00e2y treo tr\u1ea7n, khung treo bi\u1ec3n b\u1ea3ng trong nh\u00e0, ch\u1eb1ng bu\u1ed9c k\u1ebft c\u1ea5u nh\u1eb9.<br \/>\n&#8211; Trong c\u01a1 kh\u00ed nh\u1eb9: l\u00f2 xo l\u1ef1c nh\u1ecf \u2013 trung b\u00ecnh, ch\u1ed1t \u2013 k\u1eb9p \u2013 v\u00f2ng \u0111\u1ecbnh v\u1ecb, tr\u1ee5c ch\u1ed1t d\u1eabn h\u01b0\u1edbng.<br \/>\n&#8211; Trong s\u1ea3n xu\u1ea5t l\u01b0\u1edbi: l\u01b0\u1edbi h\u00e0n\/l\u01b0\u1edbi \u0111an cho k\u1ec7 si\u00eau th\u1ecb, t\u1ee7 tr\u01b0ng b\u00e0y, ch\u1eafn b\u1ea3o v\u1ec7 m\u00e1y.<br \/>\n&#8211; N\u00f4ng nghi\u1ec7p \u2013 ch\u0103n nu\u00f4i: l\u01b0\u1edbi chu\u1ed3ng tr\u1ea1i trong nh\u00e0, d\u00e2y bu\u1ed9c ch\u1ed1ng g\u1ec9 nh\u1eb9.<br \/>\n&#8211; Th\u1ef1c ph\u1ea9m (m\u00f4i tr\u01b0\u1eddng kh\u00f4, gi\u00e1n ti\u1ebfp): ph\u1ee5 ki\u1ec7n gi\u00e1 \u0111\u1ee1\/khay, chi ti\u1ebft kh\u00f4ng ti\u1ebfp x\u00fac h\u00f3a ch\u1ea5t \u2013 mu\u1ed1i; n\u1ebfu ti\u1ebfp x\u00fac tr\u1ef1c ti\u1ebfp, \u01b0u ti\u00ean 304.<\/p>\n<h3>Cam k\u1ebft ch\u1ea5t l\u01b0\u1ee3ng v\u00e0 D\u1ecbch v\u1ee5 t\u1ea1i Inox C\u01b0\u1eddng Th\u1ecbnh<\/h3>\n<p>&#8211; S\u1ea3n ph\u1ea9m ch\u00ednh h\u00e3ng, h\u1ed3 s\u01a1 CO\/CQ \u0111\u1ea7y \u0111\u1ee7, cung c\u1ea5p k\u1ebft qu\u1ea3 ki\u1ec3m tra th\u00e0nh ph\u1ea7n (PMI), \u0111\u1ed9 c\u1ee9ng theo y\u00eau c\u1ea7u.<br \/>\n&#8211; T\u1ed3n kho \u0111a d\u1ea1ng \u0111\u01b0\u1eddng k\u00ednh, b\u1ec1 m\u1eb7t s\u00e1ng \u0111\u1eb9p, \u0111\u1ed3ng \u0111\u1ec1u; c\u1eaft\/chia cu\u1ed9n theo quy c\u00e1ch \u0111\u1eb7t h\u00e0ng.<br \/>\n&#8211; B\u00e1o gi\u00e1 c\u1ea1nh tranh, minh b\u1ea1ch; h\u1ed7 tr\u1ee3 k\u1ef9 thu\u1eadt ch\u1ecdn m\u00e1c \u2013 ti\u00eau chu\u1ea9n \u2013 dung sai ph\u00f9 h\u1ee3p.<br \/>\n&#8211; \u0110\u00f3ng g\u00f3i ch\u1eafc ch\u1eafn, giao h\u00e0ng nhanh, linh ho\u1ea1t theo ti\u1ebfn \u0111\u1ed9 d\u1ef1 \u00e1n tr\u00ean to\u00e0n qu\u1ed1c.<\/p>\n","protected":false},"excerpt":{"rendered":"<p>D\u00e2y inox 201 (d\u00e2y cu\u1ed9n) c\u00f3 \u0111\u1ed9 c\u1ee9ng cao, b\u1ec1 m\u1eb7t s\u00e1ng, gi\u00e1 r\u1ebb. D\u00f9ng l\u00e0m d\u00e2y bu\u1ed9c, gia c\u00f4ng c\u00e1c chi ti\u1ebft nh\u1ecf, s\u1ea3n xu\u1ea5t l\u01b0\u1edbi v\u00e0 c\u00e1c v\u1eadt d\u1ee5ng gia \u0111\u00ecnh.<\/p>\n","protected":false},"featured_media":789,"comment_status":"open","ping_status":"closed","template":"","meta":{"_acf_changed":false},"product_brand":[],"product_cat":[71],"product_tag":[68],"class_list":["post-957","product","type-product","status-publish","has-post-thumbnail","product_cat-day-inox","product_tag-inox-201","first","instock","shipping-taxable","product-type-simple"],"acf":[],"_links":{"self":[{"href":"https:\/\/inoxcuongthinh.com\/inct\/wp\/v2\/product\/957","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/inoxcuongthinh.com\/inct\/wp\/v2\/product"}],"about":[{"href":"https:\/\/inoxcuongthinh.com\/inct\/wp\/v2\/types\/product"}],"replies":[{"embeddable":true,"href":"https:\/\/inoxcuongthinh.com\/inct\/wp\/v2\/comments?post=957"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/inoxcuongthinh.com\/inct\/wp\/v2\/media\/789"}],"wp:attachment":[{"href":"https:\/\/inoxcuongthinh.com\/inct\/wp\/v2\/media?parent=957"}],"wp:term":[{"taxonomy":"product_brand","embeddable":true,"href":"https:\/\/inoxcuongthinh.com\/inct\/wp\/v2\/product_brand?post=957"},{"taxonomy":"product_cat","embeddable":true,"href":"https:\/\/inoxcuongthinh.com\/inct\/wp\/v2\/product_cat?post=957"},{"taxonomy":"product_tag","embeddable":true,"href":"https:\/\/inoxcuongthinh.com\/inct\/wp\/v2\/product_tag?post=957"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}