{"id":964,"date":"2025-09-21T21:21:19","date_gmt":"2025-09-21T14:21:19","guid":{"rendered":"https:\/\/inoxcuongthinh.com\/san-pham\/ton-inox-430\/"},"modified":"2025-09-21T21:21:20","modified_gmt":"2025-09-21T14:21:20","slug":"ton-inox-430","status":"publish","type":"product","link":"https:\/\/inoxcuongthinh.com\/ton-inox-430\/","title":{"rendered":"T\u00f4n inox 430"},"content":{"rendered":"<h3>T\u1ed5ng quan v\u1ec1 T\u00f4n inox 430<\/h3>\n<p>T\u00f4n inox 430 l\u00e0 t\u00f4n\/t\u1ea5m inox m\u00e1c 430 thu\u1ed9c nh\u00f3m th\u00e9p kh\u00f4ng g\u1ec9 ferritic, ch\u1ee9a kho\u1ea3ng 16\u201318% Cr, g\u1ea7n nh\u01b0 kh\u00f4ng c\u00f3 Ni. Tr\u00ean th\u1ecb tr\u01b0\u1eddng, s\u1ea3n ph\u1ea9m c\u00f2n \u0111\u01b0\u1ee3c g\u1ecdi l\u00e0 SUS430 (JIS), AISI 430, ho\u1eb7c EN 1.4016 (X6Cr17). Nh\u1edd c\u01a1 t\u00ednh \u1ed5n \u0111\u1ecbnh, b\u1ec1 m\u1eb7t s\u00e1ng \u0111\u1eb9p (\u0111\u1eb7c bi\u1ec7t v\u1edbi ho\u00e0n thi\u1ec7n BA\/HL), gi\u00e1 th\u00e0nh kinh t\u1ebf v\u00e0 c\u00f3 t\u1eeb t\u00ednh, inox 430 l\u00e0 l\u1ef1a ch\u1ecdn ph\u1ed5 bi\u1ebfn cho t\u00f4n l\u1ee3p, \u1ed1p trang tr\u00ed, \u0111\u1ed3 gia d\u1ee5ng v\u00e0 c\u00e1c k\u1ebft c\u1ea5u trong m\u00f4i tr\u01b0\u1eddng kh\u00f4 r\u00e1o, \u00edt chloride. So v\u1edbi inox austenitic nh\u01b0 304\/316, kh\u1ea3 n\u0103ng ch\u1ed1ng \u0103n m\u00f2n c\u1ee7a 430 \u1edf m\u1ee9c kh\u00e1 trong \u0111i\u1ec1u ki\u1ec7n \u00f4n h\u00f2a, \u0111\u1ed5i l\u1ea1i chi ph\u00ed th\u1ea5p h\u01a1n \u0111\u00e1ng k\u1ec3.<\/p>\n<h3>B\u1ea3ng th\u00f4ng s\u1ed1 k\u1ef9 thu\u1eadt chi ti\u1ebft<\/h3>\n<table>\n<tbody>\n<tr>\n<td><strong>M\u00e1c th\u00e9p<\/strong><\/td>\n<td>SUS430 (JIS), AISI 430, EN 1.4016 (X6Cr17)<\/td>\n<\/tr>\n<tr>\n<td><strong>Ti\u00eau chu\u1ea9n<\/strong><\/td>\n<td>ASTM A240\/A240M; JIS G4304\/G4305; EN 10088-2<\/td>\n<\/tr>\n<tr>\n<td><strong>Th\u00e0nh ph\u1ea7n h\u00f3a h\u1ecdc (%)<\/strong><\/td>\n<td>C \u2264 0.08; Si \u2264 1.00; Mn \u2264 1.00; P \u2264 0.040; S \u2264 0.030; Cr 16.0\u201318.0; Ni kh\u00f4ng ch\u1ee7 \u00fd (th\u01b0\u1eddng \u2264 0.60); N \u2264 0.03<\/td>\n<\/tr>\n<tr>\n<td><strong>T\u00ednh ch\u1ea5t c\u01a1 l\u00fd<\/strong><\/td>\n<td>Kh\u1ed1i l\u01b0\u1ee3ng ri\u00eang ~7.7 g\/cm\u00b3; Gi\u1edbi h\u1ea1n ch\u1ea3y (Rp0.2) \u2265 205 MPa; \u0110\u1ed9 b\u1ec1n k\u00e9o (Rm) \u2265 450 MPa; \u0110\u1ed9 gi\u00e3n d\u00e0i \u2265 22%; \u0110\u1ed9 c\u1ee9ng \u2264 183 HB; H\u1ec7 s\u1ed1 gi\u00e3n n\u1edf ~10.4 \u00b5m\/m\u00b7K; D\u1eabn nhi\u1ec7t ~26 W\/m\u00b7K; T\u1eeb t\u00ednh: C\u00f3<\/td>\n<\/tr>\n<tr>\n<td><strong>\u0110\u1ed9 d\u00e0y ph\u1ed5 bi\u1ebfn<\/strong><\/td>\n<td>0.3\u20132.5 mm (t\u00f4n\/cu\u1ed9n c\u00e1n ngu\u1ed9i); t\u1ea5m d\u00e0y \u0111\u1ebfn 6.0 mm theo \u0111\u1eb7t h\u00e0ng<\/td>\n<\/tr>\n<tr>\n<td><strong>K\u00edch th\u01b0\u1edbc ti\u00eau chu\u1ea9n<\/strong><\/td>\n<td>Kh\u1ed5 914\/1000\/1219 mm; chi\u1ec1u d\u00e0i 2000\/2438\/3000 mm; cu\u1ed9n ID 508\/610 mm; nh\u1eadn c\u1eaft quy c\u00e1ch \u2013 d\u1eadp s\u00f3ng theo b\u1ea3n v\u1ebd<\/td>\n<\/tr>\n<tr>\n<td><strong>B\u1ec1 m\u1eb7t<\/strong><\/td>\n<td>2B, BA (Bright Annealed), No.4, HL (Hairline), ph\u1ee7 film PVC b\u1ea3o v\u1ec7; b\u1ec1 m\u1eb7t t\u00f4n s\u00f3ng m\u1ea1 m\u00e0u theo y\u00eau c\u1ea7u<\/td>\n<\/tr>\n<tr>\n<td><strong>Xu\u1ea5t x\u1ee9<\/strong><\/td>\n<td>POSCO VST (Vi\u1ec7t Nam), POSCO (H\u00e0n), YUSCO (\u0110\u00e0i Loan), TISCO\/BAOSTEEL (Trung Qu\u1ed1c), NSSC\/JFE (Nh\u1eadt), Acerinox<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<p>L\u01b0u \u00fd k\u1ef9 thu\u1eadt: Inox 430 ph\u00f9 h\u1ee3p m\u00f4i tr\u01b0\u1eddng kh\u00f4 r\u00e1o, n\u1ed9i th\u1ea5t, kh\u00ed quy\u1ec3n s\u1ea1ch. Kh\u00f4ng khuy\u1ebfn ngh\u1ecb d\u00f9ng \u1edf v\u00f9ng ven bi\u1ec3n, m\u00f4i tr\u01b0\u1eddng chloride\/axit ho\u1eb7c c\u00f4ng nghi\u1ec7p \u0103n m\u00f2n cao; khi \u0111\u00f3 n\u00ean ch\u1ecdn 304\/316.<\/p>\n<h3>So s\u00e1nh T\u00f4n inox 430 v\u1edbi c\u00e1c lo\u1ea1i ph\u1ed5 bi\u1ebfn kh\u00e1c<\/h3>\n<p>&#8211; So v\u1edbi inox 304:<br \/>\n  &#8211; Ch\u1ed1ng \u0103n m\u00f2n: 304 v\u01b0\u1ee3t tr\u1ed9i (\u0111\u1eb7c bi\u1ec7t trong m\u00f4i tr\u01b0\u1eddng \u1ea9m, chloride nh\u1eb9). 430 ch\u1ec9 ph\u00f9 h\u1ee3p m\u00f4i tr\u01b0\u1eddng \u00f4n h\u00f2a, kh\u00f4 r\u00e1o.<br \/>\n  &#8211; T\u1eeb t\u00ednh: 430 h\u00fat nam ch\u00e2m; 304 h\u1ea7u nh\u01b0 kh\u00f4ng.<br \/>\n  &#8211; H\u00e0n &#038; t\u1ea1o h\u00ecnh: 304 h\u00e0n t\u1ed1t, d\u1ebbo dai; 430 h\u00e0n\/t\u1ea1o h\u00ecnh \u1edf m\u1ee9c kh\u00e1, c\u1ea7n ki\u1ec3m so\u00e1t n\u1ee9t\/gi\u00f2n v\u00f9ng \u1ea3nh h\u01b0\u1edfng nhi\u1ec7t.<br \/>\n  &#8211; B\u1ec1 m\u1eb7t: C\u1ea3 hai \u0111\u1ec1u cho b\u1ec1 m\u1eb7t BA\/HL \u0111\u1eb9p; 430 th\u01b0\u1eddng \u0111\u01b0\u1ee3c ch\u1ecdn cho \u1ed1p trang tr\u00ed n\u1ed9i th\u1ea5t do chi ph\u00ed t\u1ed1t.<br \/>\n  &#8211; Gi\u00e1: 430 kinh t\u1ebf h\u01a1n, th\u01b0\u1eddng ti\u1ebft ki\u1ec7m \u0111\u00e1ng k\u1ec3 so v\u1edbi 304 t\u00f9y th\u1ecb tr\u01b0\u1eddng.<br \/>\n&#8211; K\u1ebft lu\u1eadn ch\u1ecdn v\u1eadt li\u1ec7u: Ch\u1ecdn 430 khi \u01b0u ti\u00ean chi ph\u00ed, y\u00eau c\u1ea7u th\u1ea9m m\u1ef9, t\u1eeb t\u00ednh, m\u00f4i tr\u01b0\u1eddng kh\u00f4 r\u00e1o. Ch\u1ecdn 304 khi c\u1ea7n ch\u1ed1ng \u0103n m\u00f2n cao h\u01a1n, d\u00f9ng ngo\u00e0i tr\u1eddi kh\u1eafc nghi\u1ec7t ho\u1eb7c ti\u1ebfp x\u00fac th\u1ef1c ph\u1ea9m\/ho\u00e1 ch\u1ea5t.<\/p>\n<h3>\u1ee8ng d\u1ee5ng th\u1ef1c t\u1ebf c\u1ee7a T\u00f4n inox 430<\/h3>\n<p>&#8211; Trong x\u00e2y d\u1ef1ng \u2013 ki\u1ebfn tr\u00fac:<br \/>\n  &#8211; T\u00f4n l\u1ee3p inox 430 cho nh\u00e0 x\u01b0\u1edfng\/n\u1ed9i \u0111\u1ecba, m\u00e1ng x\u1ed1i, m\u00e1ng c\u00e1p, \u1ed1p m\u1eb7t d\u1ef1ng n\u1ed9i th\u1ea5t, lam \u2013 n\u1eb9p trang tr\u00ed.<br \/>\n  &#8211; \u1ed0p c\u1eeda \u2013 v\u00e1ch thang m\u00e1y n\u1ed9i th\u1ea5t, \u1ed1p ch\u00e2n t\u01b0\u1eddng, bi\u1ec3n hi\u1ec7u trong nh\u00e0.<br \/>\n&#8211; \u0110\u1ed3 gia d\u1ee5ng \u2013 thi\u1ebft b\u1ecb:<br \/>\n  &#8211; V\u1ecf t\u1ee7 l\u1ea1nh, m\u00e1y r\u1eeda b\u00e1t, l\u00f2 n\u01b0\u1edbng, \u1ed1p t\u01b0\u1eddng b\u1ebfp, ch\u1ee5p h\u00fat m\u00f9i, \u1ed1ng kh\u00f3i, trang tr\u00ed b\u1ebfp.<br \/>\n&#8211; C\u01a1 kh\u00ed \u2013 \u0111i\u1ec7n:<br \/>\n  &#8211; T\u1ee7 \u0111i\u1ec7n trong nh\u00e0, n\u1eafp che m\u00e1y, v\u1ecf thi\u1ebft b\u1ecb, b\u1ea3ng \u0111i\u1ec1u khi\u1ec3n, th\u00f9ng \u2013 k\u1ec7 \u2013 b\u00e0n c\u00f4ng nghi\u1ec7p kh\u00f4.<br \/>\n&#8211; \u00d4 t\u00f4 \u2013 xe m\u00e1y:<br \/>\n  &#8211; \u1ed0p trang tr\u00ed, n\u1eb9p vi\u1ec1n, chi ti\u1ebft \u1ed1ng x\u1ea3 (ph\u1ea7n kh\u00f4ng ch\u1ecbu nhi\u1ec7t\/\u0103n m\u00f2n kh\u1eafc nghi\u1ec7t).<br \/>\n&#8211; H\u1ea1 t\u1ea7ng th\u01b0\u01a1ng m\u1ea1i:<br \/>\n  &#8211; \u1ed0p qu\u1ea7y k\u1ec7, th\u1ebb bi\u1ec3n ch\u1ec9 d\u1eabn, v\u00e1ch ng\u0103n trang tr\u00ed, tr\u1ea7n \u2013 v\u00f2m n\u1ed9i th\u1ea5t.<br \/>\n&#8211; Gia c\u00f4ng theo y\u00eau c\u1ea7u:<br \/>\n  &#8211; C\u1eaft x\u1ebb cu\u1ed9n, c\u1eaft t\u1ea5m quy c\u00e1ch, d\u1eadp s\u00f3ng t\u00f4n, ch\u1ea5n \u2013 d\u1eadp \u0111\u1ecbnh h\u00ecnh, ph\u1ee7 film b\u1ea3o v\u1ec7 b\u1ec1 m\u1eb7t.<\/p>\n<h3>Cam k\u1ebft ch\u1ea5t l\u01b0\u1ee3ng v\u00e0 D\u1ecbch v\u1ee5 t\u1ea1i Inox C\u01b0\u1eddng Th\u1ecbnh<\/h3>\n<p>&#8211; H\u00e0ng ch\u00ednh h\u00e3ng, xu\u1ea5t x\u1ee9 r\u00f5 r\u00e0ng, cung c\u1ea5p \u0111\u1ea7y \u0111\u1ee7 CO\/CQ\/MTC theo l\u00f4.<br \/>\n&#8211; Ki\u1ec3m so\u00e1t ch\u1ea5t l\u01b0\u1ee3ng \u0111\u1ea7u v\u00e0o: \u0111\u1ed9 d\u00e0y, \u0111\u1ed9 ph\u1eb3ng, b\u1ec1 m\u1eb7t, \u0111\u1ed9 c\u1ee9ng, sai l\u1ec7ch k\u00edch th\u01b0\u1edbc theo ti\u00eau chu\u1ea9n.<br \/>\n&#8211; Kho s\u1eb5n nhi\u1ec1u quy c\u00e1ch t\u00f4n inox 430 (2B\/BA\/HL), nh\u1eadn gia c\u00f4ng c\u1eaft x\u1ebb \u2013 d\u1eadp s\u00f3ng theo b\u1ea3n v\u1ebd, giao h\u00e0ng nhanh to\u00e0n qu\u1ed1c.<br \/>\n&#8211; Gi\u00e1 c\u1ea1nh tranh \u2013 t\u1ed1i \u01b0u t\u1ed5ng chi ph\u00ed d\u1ef1 \u00e1n, t\u01b0 v\u1ea5n ch\u1ecdn m\u00e1c, b\u1ec1 m\u1eb7t v\u00e0 \u0111\u1ed9 d\u00e0y ph\u00f9 h\u1ee3p \u1ee9ng d\u1ee5ng.<br \/>\n&#8211; H\u1ed7 tr\u1ee3 k\u1ef9 thu\u1eadt: khuy\u1ebfn ngh\u1ecb thi c\u00f4ng, h\u00e0n \u2013 b\u1ea3o d\u01b0\u1ee1ng \u0111\u1ec3 k\u00e9o d\u00e0i tu\u1ed5i th\u1ecd v\u1eadt li\u1ec7u.<\/p>\n","protected":false},"excerpt":{"rendered":"<p>T\u00f4n inox 430 c\u00e1n s\u00f3ng (ho\u1eb7c ph\u1eb3ng) c\u00f3 b\u1ec1 m\u1eb7t s\u00e1ng, ch\u1ecbu nhi\u1ec7t, gi\u00e1 t\u1ed1t. Th\u00edch h\u1ee3p l\u00e0m v\u00e1ch ng\u0103n, t\u1ea5m \u1ed1p trong nh\u00e0, c\u00e1c \u1ee9ng d\u1ee5ng kh\u00f4ng \u0111\u00f2i h\u1ecfi ch\u1ed1ng g\u1ec9 ngo\u00e0i tr\u1eddi.<\/p>\n","protected":false},"featured_media":796,"comment_status":"open","ping_status":"closed","template":"","meta":{"_acf_changed":false},"product_brand":[],"product_cat":[72],"product_tag":[70],"class_list":["post-964","product","type-product","status-publish","has-post-thumbnail","product_cat-ton-inox","product_tag-inox-430","first","instock","shipping-taxable","product-type-simple"],"acf":[],"_links":{"self":[{"href":"https:\/\/inoxcuongthinh.com\/inct\/wp\/v2\/product\/964","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/inoxcuongthinh.com\/inct\/wp\/v2\/product"}],"about":[{"href":"https:\/\/inoxcuongthinh.com\/inct\/wp\/v2\/types\/product"}],"replies":[{"embeddable":true,"href":"https:\/\/inoxcuongthinh.com\/inct\/wp\/v2\/comments?post=964"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/inoxcuongthinh.com\/inct\/wp\/v2\/media\/796"}],"wp:attachment":[{"href":"https:\/\/inoxcuongthinh.com\/inct\/wp\/v2\/media?parent=964"}],"wp:term":[{"taxonomy":"product_brand","embeddable":true,"href":"https:\/\/inoxcuongthinh.com\/inct\/wp\/v2\/product_brand?post=964"},{"taxonomy":"product_cat","embeddable":true,"href":"https:\/\/inoxcuongthinh.com\/inct\/wp\/v2\/product_cat?post=964"},{"taxonomy":"product_tag","embeddable":true,"href":"https:\/\/inoxcuongthinh.com\/inct\/wp\/v2\/product_tag?post=964"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}