{"id":986,"date":"2025-09-21T21:21:52","date_gmt":"2025-09-21T14:21:52","guid":{"rendered":"https:\/\/inoxcuongthinh.com\/san-pham\/inox-dap-gan-304\/"},"modified":"2025-09-21T21:21:53","modified_gmt":"2025-09-21T14:21:53","slug":"inox-dap-gan-304","status":"publish","type":"product","link":"https:\/\/inoxcuongthinh.com\/inox-dap-gan-304\/","title":{"rendered":"Inox d\u1eadp g\u00e2n 304"},"content":{"rendered":"<h3>T\u1ed5ng quan v\u1ec1 Inox d\u1eadp g\u00e2n 304<\/h3>\n<p>Inox d\u1eadp g\u00e2n 304 (c\u00f2n g\u1ecdi: t\u1ea5m inox 304 ch\u1ed1ng tr\u01b0\u1ee3t, t\u1ea5m inox 304 hoa v\u0103n n\u1ed5i) l\u00e0 t\u1ea5m th\u00e9p kh\u00f4ng g\u1ec9 m\u00e1c 304 \u0111\u01b0\u1ee3c d\u1eadp n\u1ed5i c\u00e1c h\u1ecda ti\u1ebft g\u00e2n nh\u01b0 qu\u1ea3 tr\u00e1m, 5 s\u1ecdc, x\u01b0\u01a1ng c\u00e1 nh\u1eb1m t\u0103ng ma s\u00e1t, ch\u1ed1ng tr\u01b0\u1ee3t v\u00e0 gia t\u0103ng \u0111\u1ed9 c\u1ee9ng b\u1ec1 m\u1eb7t. V\u1eadt li\u1ec7u n\u1ec1n l\u00e0 th\u00e9p kh\u00f4ng g\u1ec9 austenitic 304 (EN 1.4301) \u2013 m\u00e1c inox th\u00f4ng d\u1ee5ng nh\u1ea5t tr\u00ean th\u1ecb tr\u01b0\u1eddng nh\u1edd kh\u1ea3 n\u0103ng ch\u1ed1ng \u0103n m\u00f2n t\u1ed1t, d\u1ec5 h\u00e0n, d\u1ec5 gia c\u00f4ng v\u00e0 t\u00ednh \u1ed5n \u0111\u1ecbnh c\u01a1 h\u1ecdc.<br \/>\nT\u1ea5m d\u1eadp g\u00e2n 304 th\u01b0\u1eddng \u0111\u01b0\u1ee3c s\u1ea3n xu\u1ea5t t\u1eeb n\u1ec1n b\u1ec1 m\u1eb7t 2B\/BA, sau \u0111\u00f3 \u0111i qua tr\u1ee5c d\u1eadp (emboss\/coil-to-sheet) \u0111\u1ec3 t\u1ea1o g\u00e2n, ph\u00f9 h\u1ee3p cho c\u00e1c khu v\u1ef1c \u1ea9m \u01b0\u1edbt, d\u1ea7u m\u1ee1 ho\u1eb7c c\u1ea7n ch\u1ed1ng tr\u01b0\u1ee3t an to\u00e0n.<\/p>\n<h3>B\u1ea3ng th\u00f4ng s\u1ed1 k\u1ef9 thu\u1eadt chi ti\u1ebft<\/h3>\n<table>\n<tbody>\n<tr>\n<td><strong>M\u00e1c th\u00e9p<\/strong><\/td>\n<td>SUS304 (JIS), AISI 304, EN 1.4301<\/td>\n<\/tr>\n<tr>\n<td><strong>Ti\u00eau chu\u1ea9n<\/strong><\/td>\n<td>ASTM A240\/A480; JIS G4304\/G4305; EN 10088<\/td>\n<\/tr>\n<tr>\n<td><strong>Th\u00e0nh ph\u1ea7n h\u00f3a h\u1ecdc (%)<\/strong><\/td>\n<td>C \u2264 0.08; Cr 18.0\u201320.0; Ni 8.0\u201310.5; Mn \u2264 2.0; Si \u2264 1.0; P \u2264 0.045; S \u2264 0.03; N \u2264 0.10<\/td>\n<\/tr>\n<tr>\n<td><strong>T\u00ednh ch\u1ea5t c\u01a1 l\u00fd<\/strong><\/td>\n<td>\u0110\u1ed9 b\u1ec1n k\u00e9o \u2265 520 MPa; Gi\u1edbi h\u1ea1n ch\u1ea3y \u2265 205 MPa; \u0110\u1ed9 gi\u00e3n d\u00e0i \u2265 40%; \u0110\u1ed9 c\u1ee9ng \u2264 187 HB (\u224890 HRB); T\u1ef7 tr\u1ecdng 7.93 g\/cm\u00b3; Nhi\u1ec7t \u0111\u1ed9 l\u00e0m vi\u1ec7c gi\u00e1n \u0111o\u1ea1n t\u1ed1i \u0111a ~870\u00b0C<\/td>\n<\/tr>\n<tr>\n<td><strong>\u0110\u1ed9 d\u00e0y ph\u1ed5 bi\u1ebfn<\/strong><\/td>\n<td>0.6\u20136.0 mm (\u0111\u1ed9 d\u00e0y n\u1ec1n); g\u00e2n n\u1ed5i t\u0103ng th\u00eam ~0.2\u20130.6 mm t\u00f9y m\u1eabu; th\u00f4ng d\u1ee5ng: 0.8\/1.0\/1.2\/1.5\/2.0\/3.0 mm<\/td>\n<\/tr>\n<tr>\n<td><strong>K\u00edch th\u01b0\u1edbc ti\u00eau chu\u1ea9n<\/strong><\/td>\n<td>1000\u00d72000; 1219\u00d72438 (4\u00d78); 1250\u00d72500; 1500\u00d73000 mm; Kh\u1ed5 cu\u1ed9n 1000\/1219\/1500 mm; C\u1eaft x\u1ebb theo k\u00edch th\u01b0\u1edbc y\u00eau c\u1ea7u<\/td>\n<\/tr>\n<tr>\n<td><strong>B\u1ec1 m\u1eb7t<\/strong><\/td>\n<td>N\u1ec1n 2B\/BA\/No.1; D\u1eadp g\u00e2n: qu\u1ea3 tr\u00e1m, 5 s\u1ecdc, x\u01b0\u01a1ng c\u00e1, h\u1ea1t d\u1ebb; T\u00f9y ch\u1ecdn ph\u1ee7 film PE m\u1ed9t m\u1eb7t; M\u00e9p m\u00e0i bavia<\/td>\n<\/tr>\n<tr>\n<td><strong>Xu\u1ea5t x\u1ee9<\/strong><\/td>\n<td>POSCO (VN\/HQ), BAOSTEEL\/TISCO (CN), YUSCO (TW), Jindal (IN), Acerinox (EU) \u2013 \u0111\u1ea7y \u0111\u1ee7 CO\/CQ, truy xu\u1ea5t heat number<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<h3>So s\u00e1nh Inox d\u1eadp g\u00e2n 304 v\u1edbi c\u00e1c lo\u1ea1i ph\u1ed5 bi\u1ebfn kh\u00e1c<\/h3>\n<p>&#8211; So v\u1edbi inox d\u1eadp g\u00e2n 201:<br \/>\n  &#8211; Ch\u1ed1ng \u0103n m\u00f2n: 304 v\u01b0\u1ee3t tr\u1ed9i nh\u1edd h\u00e0m l\u01b0\u1ee3ng Ni cao (8\u201310.5%) v\u00e0 Cr 18\u201320%; 201 d\u00f9ng Mn thay Ni n\u00ean k\u00e9m b\u1ec1n trong m\u00f4i tr\u01b0\u1eddng \u1ea9m\/mu\u1ed1i\/axit nh\u1eb9.<br \/>\n  &#8211; Gi\u00e1: 201 r\u1ebb h\u01a1n kho\u1ea3ng 10\u201325% t\u00f9y th\u1eddi \u0111i\u1ec3m; 304 gi\u00e1 cao h\u01a1n nh\u01b0ng tu\u1ed5i th\u1ecd v\u00e0 chi ph\u00ed v\u00f2ng \u0111\u1eddi th\u1ea5p h\u01a1n trong m\u00f4i tr\u01b0\u1eddng kh\u1eafc nghi\u1ec7t.<br \/>\n  &#8211; \u1ee8ng d\u1ee5ng: 304 ph\u00f9 h\u1ee3p ngo\u00e0i tr\u1eddi, g\u1ea7n bi\u1ec3n, ng\u00e0nh th\u1ef1c ph\u1ea9m; 201 ph\u00f9 h\u1ee3p kh\u00f4ng gian kh\u00f4 r\u00e1o trong nh\u00e0, \u00edt \u0103n m\u00f2n.<br \/>\n  &#8211; T\u1eeb t\u00ednh: C\u1ea3 304 v\u00e0 201 \u1edf tr\u1ea1ng th\u00e1i \u1ee7 th\u01b0\u1eddng g\u1ea7n nh\u01b0 kh\u00f4ng nhi\u1ec5m t\u1eeb; c\u00f3 th\u1ec3 h\u01a1i nhi\u1ec5m t\u1eeb sau khi c\u00e1n ngu\u1ed9i\/d\u1eadp g\u00e2n \u2013 l\u00e0 hi\u1ec7n t\u01b0\u1ee3ng b\u00ecnh th\u01b0\u1eddng.<\/p>\n<h3>\u1ee8ng d\u1ee5ng th\u1ef1c t\u1ebf c\u1ee7a Inox d\u1eadp g\u00e2n 304<\/h3>\n<p>&#8211; Trong ng\u00e0nh th\u1ef1c ph\u1ea9m: s\u00e0n khu ch\u1ebf bi\u1ebfn \u01b0\u1edbt, l\u1ed1i \u0111i ch\u1ed1ng tr\u01b0\u1ee3t, b\u1eadc thang, b\u1ec7 thao t\u00e1c.<br \/>\n&#8211; X\u00e2y d\u1ef1ng \u2013 ki\u1ebfn tr\u00fac: s\u00e0n k\u1ef9 thu\u1eadt, b\u1eadc c\u1ea7u thang, ram d\u1ed1c, chi\u1ebfu ngh\u1ec9, \u1ed1p b\u1ea3o v\u1ec7 g\u00f3c t\u01b0\u1eddng.<br \/>\n&#8211; Giao th\u00f4ng \u2013 v\u1eadn t\u1ea3i: s\u00e0n xe t\u1ea3i\/xe bu\u00fdt, th\u00f9ng xe, s\u00e0n container, b\u1ebfn b\u00e3i.<br \/>\n&#8211; H\u00e0ng h\u1ea3i \u2013 d\u1ea7u kh\u00ed: boong t\u00e0u, c\u1ea7u c\u1ea3ng, l\u1ed1i \u0111i tr\u00ean bi\u1ec3n, khu v\u1ef1c phun s\u01b0\u01a1ng mu\u1ed1i.<br \/>\n&#8211; Thang m\u00e1y \u2013 c\u01a1 \u0111i\u1ec7n: s\u00e0n cabin, s\u00e0n ph\u00f2ng m\u00e1y, h\u00e0nh lang k\u1ef9 thu\u1eadt.<br \/>\n&#8211; H\u1ea1 t\u1ea7ng \u2013 nh\u00e0 m\u00e1y: n\u1eafp h\u1ed1 ga, s\u00e0n thao t\u00e1c, l\u1ed1i \u0111i tr\u00ean cao, khu v\u1ef1c c\u00f3 d\u1ea7u m\u1ee1\/\u1ea9m \u01b0\u1edbt.<br \/>\n&#8211; Ch\u0103n nu\u00f4i \u2013 th\u1ee7y s\u1ea3n: s\u00e0n khu r\u1eeda, khu s\u01a1 ch\u1ebf, d\u1ec5 v\u1ec7 sinh, s\u1ea1ch s\u1ebd.<\/p>\n<h3>Cam k\u1ebft ch\u1ea5t l\u01b0\u1ee3ng v\u00e0 D\u1ecbch v\u1ee5 t\u1ea1i Inox C\u01b0\u1eddng Th\u1ecbnh<\/h3>\n<p>&#8211; H\u00e0ng ch\u00ednh h\u00e3ng, \u0111\u1ea7y \u0111\u1ee7 CO\/CQ, truy xu\u1ea5t ngu\u1ed3n g\u1ed1c theo heat number; ki\u1ec3m tra PMI\/th\u00e0nh ph\u1ea7n theo y\u00eau c\u1ea7u.<br \/>\n&#8211; T\u1ed3n kho \u0111a d\u1ea1ng m\u00e1c, m\u1eabu g\u00e2n v\u00e0 k\u00edch th\u01b0\u1edbc; c\u1eaft l\u1ebb theo quy c\u00e1ch, ch\u1ea5n \u2013 gia c\u00f4ng ho\u00e0n thi\u1ec7n nhanh.<br \/>\n&#8211; Quy tr\u00ecnh ki\u1ec3m so\u00e1t ch\u1ea5t l\u01b0\u1ee3ng nghi\u00eam ng\u1eb7t: \u0111\u00fang m\u00e1c \u2013 \u0111\u00fang \u0111\u1ed9 d\u00e0y \u2013 \u0111\u00fang b\u1ec1 m\u1eb7t; \u0111\u00f3ng g\u00f3i ph\u1ee7 film, pallet g\u1ed7, b\u1ea3o v\u1ec7 c\u1ea1nh.<br \/>\n&#8211; B\u00e1o gi\u00e1 c\u1ea1nh tranh theo ng\u00e0y, chi\u1ebft kh\u1ea5u theo s\u1ed1 l\u01b0\u1ee3ng, xu\u1ea5t h\u00f3a \u0111\u01a1n VAT, giao h\u00e0ng nhanh t\u1ea1i mi\u1ec1n B\u1eafc v\u00e0 c\u00e1c t\u1ec9nh.<br \/>\n&#8211; T\u01b0 v\u1ea5n k\u1ef9 thu\u1eadt mi\u1ec5n ph\u00ed: l\u1ef1a ch\u1ecdn \u0111\u1ed9 d\u00e0y t\u1ed1i \u01b0u theo t\u1ea3i tr\u1ecdng, m\u00f4i tr\u01b0\u1eddng, ti\u00eau chu\u1ea9n l\u1eafp \u0111\u1eb7t an to\u00e0n.<\/p>\n","protected":false},"excerpt":{"rendered":"<p>Inox d\u1eadp g\u00e2n 304 (t\u1ea5m ch\u1ed1ng tr\u01b0\u1ee3t) l\u00e0 l\u1ef1a ch\u1ecdn ph\u1ed5 bi\u1ebfn nh\u1ea5t cho s\u00e0n xe t\u1ea3i, l\u1ed1i \u0111i nh\u00e0 x\u01b0\u1edfng, s\u00e0n kho l\u1ea1nh nh\u1edd kh\u1ea3 n\u0103ng ch\u1ed1ng g\u1ec9 v\u00e0 ch\u1ecbu l\u1ef1c t\u1ed1t.<\/p>\n","protected":false},"featured_media":818,"comment_status":"open","ping_status":"closed","template":"","meta":{"_acf_changed":false},"product_brand":[],"product_cat":[79],"product_tag":[69],"class_list":["post-986","product","type-product","status-publish","has-post-thumbnail","product_cat-inox-dap-gan","product_tag-inox-304","first","instock","shipping-taxable","product-type-simple"],"acf":[],"_links":{"self":[{"href":"https:\/\/inoxcuongthinh.com\/inct\/wp\/v2\/product\/986","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/inoxcuongthinh.com\/inct\/wp\/v2\/product"}],"about":[{"href":"https:\/\/inoxcuongthinh.com\/inct\/wp\/v2\/types\/product"}],"replies":[{"embeddable":true,"href":"https:\/\/inoxcuongthinh.com\/inct\/wp\/v2\/comments?post=986"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/inoxcuongthinh.com\/inct\/wp\/v2\/media\/818"}],"wp:attachment":[{"href":"https:\/\/inoxcuongthinh.com\/inct\/wp\/v2\/media?parent=986"}],"wp:term":[{"taxonomy":"product_brand","embeddable":true,"href":"https:\/\/inoxcuongthinh.com\/inct\/wp\/v2\/product_brand?post=986"},{"taxonomy":"product_cat","embeddable":true,"href":"https:\/\/inoxcuongthinh.com\/inct\/wp\/v2\/product_cat?post=986"},{"taxonomy":"product_tag","embeddable":true,"href":"https:\/\/inoxcuongthinh.com\/inct\/wp\/v2\/product_tag?post=986"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}